Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Graphite Cloth Composite". Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.32 - 1.39 g/cc
0.0477 - 0.0502 lb/in³
Average value: 1.35 g/cc Grade Count:3
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 68.7 - 80.0 MPa
9970 - 11600 psi
Average value: 75.3 MPa Grade Count:3
Flexural Yield Strength 123 - 139 MPa
17800 - 20200 psi
Average value: 133 MPa Grade Count:3
Flexural Modulus 8.07 - 11.7 GPa
1170 - 1700 ksi
Average value: 10.2 GPa Grade Count:3
Compressive Yield Strength 75.2 - 91.0 MPa
10900 - 13200 psi
Average value: 81.8 MPa Grade Count:3
Compressive Modulus 12.1 - 14.7 GPa
1750 - 2130 ksi
Average value: 13.4 GPa Grade Count:3