Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Overview of materials for Polypropylene w/ 50% Calcium Carbonate

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 50% Calcium Carbonate
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Overview of materials for Polypropylene w/ 50% Calcium Carbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This property data is a summary of similar materials in the MatWeb database for the category "Polypropylene w/ 50% Calcium Carbonate". Specific grades with calcium carbonate content between 45% and 54% are included. Each property range of values reported is minimum and maximum values of appropriate MatWeb entries. The comments report the average value, and number of data points used to calculate the average. The values are not necessarily typical of any specific grade, especially less common values and those that can be most affected by additives or processing methods.
Physical Properties Metric English Comments
Density 1.24 - 1.84 g/cc
0.0448 - 0.0665 lb/in³
Average value: 1.45 g/cc Grade Count:8
Melt Flow 0.350 - 30.0 g/10 min
0.350 - 30.0 g/10 min
Average value: 11.6 g/10 min Grade Count:6
Mechanical Properties Metric English Comments
Elongation at Break 50.0 - 469 %
50.0 - 469 %
Average value: 251 % Grade Count:3
Flexural Modulus 1.60 - 2.96 GPa
232 - 430 ksi
Average value: 2.35 GPa Grade Count:5
Izod Impact, Notched (ISO) 4.98 - 4.98 kJ/m²

@Temperature -40.0 - -40.0 °C
2.37 - 2.37 ft-lb/in²

@Temperature -40.0 - -40.0 °F
Average value: 4.98 kJ/m² Grade Count:1
Gardner Impact 12.4 - 19.0 J
9.15 - 14.0 ft-lb
Average value: 15.8 J Grade Count:4
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 93.3 - 107 °C
200 - 225 °F
Average value: 102 °C Grade Count:3
Users viewing this material also viewed the following: