P & P Technology CB 70 Carbon Loaded Silicone

Category Polymer , Thermoset , Silicone
Manufacturer P & P Technology
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF P & P Technology CB 70 Carbon Loaded Silicone.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Applications: Electrically conductive grades which when properly catalyzed can be considered for applications requiring conductivity such as EMI gaskets, conductive sheaths for ignition cable core, electronic keyboard contacts, etc.Information provided by P & P Technology
Physical Properties Metric English Comments
Specific Gravity 1.17 g/cc
1.17 g/cc
DIN 53479-A
Mechanical Properties Metric English Comments
Hardness, Shore A 73
73
DIN 53505-A
Tensile Strength 6.00 MPa
870 psi
DIN 53504-S1
Elongation at Break 210 %
210 %
DIN 53504-S1
Tear Strength 12.0 kN/m
68.5 pli
ASTM D624B
Compression Set 33 %
33 %
DIN ISO815-B
Electrical Properties Metric English Comments
Volume Resistivity 1.5 ohm-cm
1.5 ohm-cm
DIN IEC93