P & P Technology EC-S Pure Silver Loaded Silicone

Category Polymer , Thermoset , Silicone
Manufacturer P & P Technology
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF P & P Technology EC-S Pure Silver Loaded Silicone.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
P & P Technology material reference EC-S is a silicone elastomer with Silver conductive filler. It is tan in color. The material is specially compounded to offer excellent physical and electrical properties over an effective temperature range of –50 to + 150°C. Silicone offers excellent performance over a wide temperature range with good resistance to chemicals and weathering. Its resistance to mineral based fluids is limited, but it has good splash contact resistance to most mineral oils and greases.Information provided by P & P Technology
Physical Properties Metric English Comments
Specific Gravity 3.20 g/cc
3.20 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength 1.25 MPa
181 psi
ASTM D412
Elongation at Break >= 100 %
>= 100 %
ASTM D412
Tear Strength >= 0.000875 kN/m
>= 0.00499 pli
Compression Set <= 30 %

@Temperature 100 °C,
Time 259000 sec
<= 30 %

@Temperature 212 °F,
Time 72.0 hour
ASTM D395
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 150 °C
302 °F
Minimum Service Temperature, Air -50.0 °C
-58.0 °F
Electrical Properties Metric English Comments
Volume Resistivity <= 0.0020 ohm-cm
<= 0.0020 ohm-cm
Mil-G-83528
Shielding Effectiveness 70 dB

@Frequency 200000 Hz
70 dB

@Frequency 200000 Hz
Mil-G-83528/Mil std 285
115 dB

@Frequency 1.00e+8 Hz
115 dB

@Frequency 1.00e+8 Hz
Mil-G-83528/Mil std 285
115 dB

@Frequency 5.00e+8 Hz
115 dB

@Frequency 5.00e+8 Hz
Mil-G-83528/Mil std 285
115 dB

@Frequency 2.00e+9 Hz
115 dB

@Frequency 2.00e+9 Hz
Mil-G-83528/Mil std 285
115 dB

@Frequency 1.00e+10 Hz
115 dB

@Frequency 1.00e+10 Hz
Mil-G-83528/Mil std 285