Electrical Properties | Metric | English | Comments |
---|---|---|---|
Shielding Effectiveness | 70 dB @Frequency 1.00e+10 Hz |
70 dB @Frequency 1.00e+10 Hz |
1/8 thickness |
PolyOne Stat-Tech™ NN-40CF/000 NH FRV0 Natural Polyamide 66 (Nylon 66) Stat-Tech™ Electrically Conductive Compounds are specifically engineered to provide anti-static, ESD and RFI/EMI shielding performance for critical electronic equipment applications. These compound.. |
|||
Shielding Effectiveness | 70 dB @Frequency 200000 Hz |
70 dB @Frequency 200000 Hz |
Mil-G-83528/Mil std 285 |
P & P Technology EC-S Pure Silver Loaded Silicone P & P Technology material reference EC-S is a silicone elastomer with Silver conductive filler. It is tan in color. The material is specially compounded to offer excellent physical and electrical p.. |
|||
Shielding Effectiveness | >= 70 dB @Frequency 200000 Hz |
>= 70 dB @Frequency 200000 Hz |
H Field; MIL-DTL-83528 Para.4.6.12 |
Parker Chomerics CHO-SEAL 1212 Conductive Elastomer High strength, hard (80 shore A) material for waveguide, choke, cover, and flanges with grooves for EMI and pressure sealing.Molded onlyRoHS Compliant Information provided by Chomerics |
|||
Shielding Effectiveness | >= 70 dB @Frequency 200000 Hz |
>= 70 dB @Frequency 200000 Hz |
H Field; MIL-DTL-83528 Para.4.6.12 |
Parker Chomerics CHO-SEAL 1224 Conductive Elastomer Highest shielding effectiveness and through conductivity performance; higher physical properties; excellent processing; also available in a fabric reinforced format.Molded onlyRoHS CompliantInformat.. |
|||
Shielding Effectiveness | >= 70 dB @Frequency 200000 Hz |
>= 70 dB @Frequency 200000 Hz |
H Field; MIL-DTL-83528 Para.4.6.12 |
Parker Chomerics CHO-SEAL 1239 Conductive Elastomer Material for waveguide choke, cover, and flange EMI shielding and pressure sealing; maximum heat transfer and minimum outgassing; hard (80 Shore A), high-strength material; available with raised lip.. |
|||
Shielding Effectiveness | >= 70 dB @Frequency 2.00e+9 Hz |
>= 70 dB @Frequency 2.00e+9 Hz |
Plane Wave; Method 3, CHO-TM-TP09 |
Parker Chomerics CHO-SEAL® 1270 Conductive Elastomer Description: Material of choice for high-end commercial applications; superior performance, in non-corrosive environments; tear trim compression and injection molding. A low durometer hardness elast.. |
|||
Shielding Effectiveness | >= 70 dB @Frequency 1.00e+10 Hz |
>= 70 dB @Frequency 1.00e+10 Hz |
Plane Wave; Method 3, CHO-TM-TP09 |
Parker Chomerics CHO-SEAL® 1270 Conductive Elastomer Description: Material of choice for high-end commercial applications; superior performance, in non-corrosive environments; tear trim compression and injection molding. A low durometer hardness elast.. |
|||
Shielding Effectiveness | >= 70 dB @Frequency 2.00e+9 Hz |
>= 70 dB @Frequency 2.00e+9 Hz |
Plane Wave; Method 1, CHO-TM-TP08 |
Parker Chomerics CHO-SEAL® 6330 Conductive Elastomer Description: Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact. A low durometer hardness elastomer, i.. |
|||
Shielding Effectiveness | >= 70 dB @Frequency 1.00e+10 Hz |
>= 70 dB @Frequency 1.00e+10 Hz |
Plane Wave; Method 1, CHO-TM-TP08 |
Parker Chomerics CHO-SEAL® 6330 Conductive Elastomer Description: Good performance in moderately corrosive environments; material of choice for flange finishes needing “bite-through” for good electrical contact. A low durometer hardness elastomer, i.. |
|||
Shielding Effectiveness | 70 dB @Frequency 1.00e+10 Hz |
70 dB @Frequency 1.00e+10 Hz |
2mm x 6mm |
Parker Chomerics SOFT-SHIELD® 4850-STRIP Low-Closure Force Strip Gasket Description: SOFT-SHIELD® 4850-STRIP multi-planar, Z-axis conductive strip gaskets are a new, convenient form of the successful 4850 EMI sheet gasket. These strip gaskets provide EMI shielding in t.. |
|||
Shielding Effectiveness | 70 - 80 dB @Frequency 2.00e+7 - 1.00e+10 Hz |
70 - 80 dB @Frequency 2.00e+7 - 1.00e+10 Hz |
CHO-TM-TP08 |
Parker Chomerics SOFT-SHIELD® 4850-STRIP Low-Closure Force Strip Gasket Description: SOFT-SHIELD® 4850-STRIP multi-planar, Z-axis conductive strip gaskets are a new, convenient form of the successful 4850 EMI sheet gasket. These strip gaskets provide EMI shielding in t.. |
|||
Shielding Effectiveness | 70 dB @Frequency 100000 Hz |
70 dB @Frequency 100000 Hz |
H-Field |
Parker Chomerics Tecknit Consil®-R 855 Pure Silver-Filled Silicone Elastomer Description: CONSIL-RHT 855 is a pure silver-filled silicone elastomer ideal for applications where high temperature is a concernTypical Applications: CONSIL-RHT 855 silicone is used throughout indu.. |
|||
Shielding Effectiveness | >= 70 dB @Frequency 100000 Hz |
>= 70 dB @Frequency 100000 Hz |
H-Field |
Parker Chomerics Tecknit Consil®-R 856 Pure Silver-Filled Silicone Elastomer Description: CONSIL-R 856 offers the lowest durometer available for pure silver-filled elastomerTypical Applications: CONSIL-R is designed for use in low to moderate pressure applicationsInformation.. |
|||
Shielding Effectiveness | >= 70 dB @Frequency 100000 Hz |
>= 70 dB @Frequency 100000 Hz |
H-Field |
Parker Chomerics Tecknit Consil®-R 857 Pure Silver-Filled Silicone Elastomer Description: CONSIL-R 857 provides similar properties as 856, with a high durometerTypical Applications: CONSIL-R is designed for use in low to moderate pressure applicationsInformation provided by .. |
|||
Shielding Effectiveness | 70 dB @Frequency 1.00e+9 Hz |
70 dB @Frequency 1.00e+9 Hz |
Plane Wave |
Parker Chomerics Tecknit Consil®-V 751 Extruded Silver-Filled Silicone Elastomer Description: Consil-V is an extruded silicone elastomer filled with silver-plated inert particles. The V-shape cross section is ideally suited for applications requiring low closure force gasketing... |
|||
Shielding Effectiveness | 70 dB @Frequency 1.00e+9 Hz |
70 dB @Frequency 1.00e+9 Hz |
|
Parker Chomerics SOFT-SHIELD® 2000 Low Closure Force, Foam Core EMI Gasket Description: SOFT-SHIELD® 2000 Series gaskets consist of silver-plated nylon yarn knitted as the outer layer over a highly compressible, thermoplastic EPDM foam core. Through a special treatment pr.. |
|||
Shielding Effectiveness | >= 70 dB @Frequency 200000 Hz |
>= 70 dB @Frequency 200000 Hz |
H Field; MIL-DLT-83528 Para.4.6.12 |
Parker Chomerics CHO-SEAL 1215 Conductive Elastomer Resists highest level of EMP induced current; military gasket of choice in non-corrosive environments; excellent processing for molding and extrusion. Molded and ExtrudedRoHS Compliant Information p.. |
|||
Shielding Effectiveness | >= 70 dB @Frequency 200000 Hz |
>= 70 dB @Frequency 200000 Hz |
H Field; MIL-DTL-83528 Para.4.6.12 |
Parker Chomerics CHO-SEAL 1217 Conductive Elastomer Resists highest level of EMP induced current; military gasket of choice in non-corrosive environments; excellent processing for molding and extrusion. Molded and ExtrudedRoHS Compliant Information p.. |
|||
Shielding Effectiveness | >= 70 dB @Frequency 200000 Hz |
>= 70 dB @Frequency 200000 Hz |
H Field; MIL-DTL-83528 Para.4.6.12 |
Parker Chomerics CHO-SEAL 1221 Conductive Elastomer Highest shielding effectiveness and through conductivity performance; higher physical properties; excellent processing; also available in a fabric reinforced format.Molded onlyRoHS CompliantInformat.. |
|||
Shielding Effectiveness | 70 dB @Frequency 1.00e+10 Hz |
70 dB @Frequency 1.00e+10 Hz |
|
Parker Chomerics CHO-SHIELD® 2044 Nickel-Filled Acrylic Coating for EMI Shielding Description: CHO-SHIELD® 2044 is an electrically conductive, one-component nickel-filled acrylic coating that is especially formulated for application on plastics to provide modest EMI shielding. C.. |