PPT BP18 NiZn Ferrite Powder

Category Ceramic , Oxide
Manufacturer Powder Processing & Technology LLC (PPT)
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PPT BP18 NiZn Ferrite Powder.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Uses: EMI Suppressors, Wave Absorbing Tiles, Impeders, Multi-Hole Connectors, Inductors, Transformers, Converters, Choke Coils, AntennasElectromagnetic characteristics were tested on toroid with a HP4294A.
Physical Properties Metric English Comments
Bulk Density 1.50 g/cc
0.0542 lb/in³
typical
Particle Size 120 µm
120 µm
median granule size
Thermal Properties Metric English Comments
Shrinkage 12 %
12 %
Electrical Properties Metric English Comments
Electrical Resistivity 1e+7 ohm-cm
1e+7 ohm-cm
Magnetic Coercive Force, Hc 8.9 Oe
8.9 Oe
Magnetic Remanence, Br 800 Gauss
800 Gauss
Curie Temperature 500 °C
932 °F
Processing Properties Metric English Comments
Moisture Content 0.30 %
0.30 %
Sintering Temperature 1260 °C

@Time 7200 sec
2300 °F

@Time 2.00 hour
Descriptive Properties Value Comments
Flux Density Bs 1800 Gauss
Field Strength = 40 Oe
Initial Permeability, µi 18
Q Factor (w/ 10 turns) 250
10 MHz