Electrical Properties | Metric | English | Comments |
---|---|---|---|
Electrical Resistivity | 1e+7 ohm-cm | 1e+7 ohm-cm | |
PPT BP80 NiZn Ferrite Powder Uses: EMI Suppressors, Wave Absorbing Tiles, Impeders, Multi-Hole Connectors, Inductors, Transformers, Converters, Choke Coils, AntennasElectromagnetic characteristics were tested on toroid with a H.. |
|||
Electrical Resistivity | 1e+7 ohm-cm | 1e+7 ohm-cm | at 100V |
PPT FP215 Fully Sintered Ferrite Powder Fully sintered NiZn ferrite, MnZn ferrite, and MgZn ferrite powders are available. Spherical or irregular particle shapes in custom particle sizes are available, ranging from sub-micron to a few hu.. |
|||
Electrical Resistivity | 1e+7 ohm-cm | 1e+7 ohm-cm | |
PPT BP1500 NiZn Ferrite Powder Uses: EMI Suppressors, Wave Absorbing Tiles, Impeders, Multi-Hole Connectors, Inductors, Transformers, Converters, Choke Coils, AntennasElectromagnetic characteristics were tested on toroid with a H.. |
|||
Electrical Resistivity | 1e+7 ohm-cm | 1e+7 ohm-cm | |
PPT BP2000 NiZn Ferrite Powder Uses: EMI Suppressors, Wave Absorbing Tiles, Impeders, Multi-Hole Connectors, Inductors, Transformers, Converters, Choke Coils, AntennasElectromagnetic characteristics were tested on toroid with a H.. |
|||
Electrical Resistivity | 1e+7 ohm-cm | 1e+7 ohm-cm | |
PPT BP18 NiZn Ferrite Powder Uses: EMI Suppressors, Wave Absorbing Tiles, Impeders, Multi-Hole Connectors, Inductors, Transformers, Converters, Choke Coils, AntennasElectromagnetic characteristics were tested on toroid with a H.. |
|||
Electrical Resistivity | 1e+7 ohm-cm | 1e+7 ohm-cm | |
PPT BP40 NiZn Ferrite Powder Uses: EMI Suppressors, Wave Absorbing Tiles, Impeders, Multi-Hole Connectors, Inductors, Transformers, Converters, Choke Coils, AntennasElectromagnetic characteristics were tested on toroid with a H.. |