Material Notes:
Description: Paratherm MR® is a mid-range heat transfer fluid. It is efficient across the temperature range, thermally stable and cost-effective. Non-aromatic and non-toxic, the fluid is safe to use and is easy to dispose. Used or contaminated fluid can be safely combined with spent lubricating oils and recycled locally. It is designed for a broad variety of applications such as batch reactors, laminating lines and plastics mold tenoerature control. Information provided by Paratherm Corporation.
Physical Properties Metric English Comments
Density 0.803 g/cc

@Temperature 23.9 °C
0.0290 lb/in³

@Temperature 75.0 °F
Molecular Weight 230 g/mol
230 g/mol
average; ASTM D2502
Thermal Properties Metric English Comments
Heat of Vaporization 293.8 J/g
126.4 BTU/lb
calculated
CTE, linear 782 µm/m-°C

@Temperature 20.0 °C
435 µin/in-°F

@Temperature 68.0 °F
Boiling Point 301 - 327 °C
574 - 621 °F
atmospheric boiling range, 10% fraction to 90% fraction; ASTM D1160
Maximum Service Temperature, Air 288 °C
550 °F
optimum use range
<= 316 °C
<= 600 °F
max. recommended film temperature
Minimum Service Temperature, Air -1.11 °C
30.0 °F
optimum use range
Pour Point -62.2 °C
-80.0 °F
ASTM D97
Flash Point 149 °C
300 °F
coc; ASTM D92
Descriptive Properties Value Comments
Appearance transparent, bright water white
Autoignition 621°F
ASTM E659
Feedstock hydrocarbon
Fire point 325°F
ASTM D92, coc
Odor slight
Pumpability -76°F
centrifugal at 2000 centipoise
Total Acid Number 0.01
ASTM D664