Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Parker Chomerics CHO-BOND 1053, Part B Silicone Rubber Mixture

Category Polymer , Thermoset , Silicone
Manufacturer Parker Chomerics
Trade Name CHO-BOND
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics CHO-BOND 1053, Part B Silicone Rubber Mixture.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity >= 1.00 g/cc
>= 1.00 g/cc
Thermal Properties Metric English Comments
Flash Point >= 93.3 °C
>= 200 °F
Descriptive Properties Value Comments
Calcium Carbonate wt. % Max 10
Physical Form Beige liquid, little or no odor
Silica, Crystalline Quartz % <60
Silicone Resin % <70
Users viewing this material also viewed the following: