Parker Chomerics CHO-BOND 116-19L Silicone Rubber Mixture

Category Polymer , Adhesive , Thermoset , Silicone
Manufacturer Parker Chomerics
Trade Name CHO-BOND
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics CHO-BOND 116-19L Silicone Rubber Mixture.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity 3.80 g/cc
3.80 g/cc
Solubility in Water 0.00 %
0.00 %
Insoluble
Thermal Properties Metric English Comments
Flash Point >= 93.3 °C
>= 200 °F
Component Elements Properties Metric English Comments
Copper, Cu 70 - 85 %
70 - 85 %
Silver, Ag 1.0 - 15 %
1.0 - 15 %
Descriptive Properties Value Comments
Color Gray
Physical Form Gray paste with sweet odor.
Silicone Resin % <30