Parker Chomerics CHO-BOND 2166 Part A Silicone

Category Polymer , Adhesive , Thermoset , Silicone
Manufacturer Parker Chomerics
Trade Name CHO-BOND
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Parker Chomerics CHO-BOND 2166 Part A Silicone.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by Chomerics
Physical Properties Metric English Comments
Specific Gravity 1.00 g/cc
1.00 g/cc
Solubility in Water 0.00 %
0.00 %
Insoluble
Thermal Properties Metric English Comments
Flash Point >= 93.3 °C
>= 200 °F
Descriptive Properties Value Comments
Color White
Fluorosilicone Proprietary wt. % Max 50
Octamethyltrisiloxane wt. % Max 10
Physical Form White paste with a mild odor.
Silica, Crystalline Quartz wt. % Max 60