Pau Tai Dibasic lead phosphite, Monomer Stabilizer

Category Other Engineering Material , Additive/Filler for Polymer
Manufacturer Pau Tai Industrial Corp.
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Pau Tai Dibasic lead phosphite, Monomer Stabilizer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Excellent dispersibility and heat stability. Powerful continuous reducing power, excellent resistance to elements, ageing resistance and heat stability.Applications: Wire is wrapped,soft white opaque products.
Physical Properties Metric English Comments
Specific Gravity 6.90 g/cc
6.90 g/cc
Particle Mesh Size 325 Mesh
325 Mesh
passed 99.7%
Processing Properties Metric English Comments
Moisture Content <= 0.30 %
<= 0.30 %
Descriptive Properties Value Comments
Appearance White micropowder
Metal Content % 88+/- 1%