Physical Properties | Metric | English | Comments |
---|---|---|---|
Particle Mesh Size | 325 Mesh | 325 Mesh | 100% through |
Manufacturing Insight EFR-3 Enhanced Fire Retardant Additive EFR-3 is ideal for incorporation into unreinforced thermoset resin systems, including coatings and foams, potting compounds as well as electronic laminates and other similar applications. EFR-3 has .. |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | 0.5% retained |
Imerys Allenâ„¢ G Kaolin Allen G is an intermediate-grained kaolin used as a suspension aid in ceramic glazes.Information provided by Imerys |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | 0.5% retained |
Imerys Allenâ„¢ R Kaolin Allen is an intermediate-grained kaolin suitable for use as a filler in soft rubber products, plastic compounds, adhesives, protective coatings and similar applications.Information provided by Imery.. |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | 2% retained |
Imerys Hamiltonâ„¢ Kaolin Hamilton is a fine-grained kaolin with low alkali content and high PCE. These properties make for ideal air-set refractory mortars. Halloysite content provides excellent suspension and trowel abilit.. |
|||
Particle Mesh Size | >= 325 Mesh | >= 325 Mesh | 0.9765 |
Gromax Melamine (Fine Grade) China KInformation provided by Gromax Enterprises Corp. |
|||
Particle Mesh Size | >= 325 Mesh | >= 325 Mesh | 0.1525 |
Gromax Standard GB9567-97 China SInformation provided by Gromax Enterprises Corp. |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | 0.005% Retained |
KaMin KaMin® 2000C Kaolin Clay - Calcined Highest brightness, smallest particle size, calcined kaolin clay, more cost -effective Ti02 extender than KaMin® 70C.Industry: Paint & CoatingsUses: Architectural Coatings, Industrial Coatings, F.. |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | 0.1% Retained |
KaMin Nucap® 190W Kaolin Clay - Surface Treated Reinforcing filler/extender for elastomeric systems. Nucap®190W is a high brightness treated kaolin used in white roofing membranes and white sidewalls. Silane treated clays mix in quicker and ma.. |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | Powder |
Lucas-Milhaupt Lucanex 721 Active Metal Brazing Brazing Paste Blended with Ti for active metal brazing of ceramics.Information provided by Lucas-Milhaupt, Inc.Alloy compositions are for filler metal powder in Lucanex paste |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | 0.01% Retained |
KaMin Polyfil® 80 Kaolin Clay - Calcined Higher brightness, medium particle size, calcined kaolin.Industry: Rubber & PlasticUses: Non-Black Rubber, General Rubber GoodsInformation provided by KaMin LLC. |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | 0.005% Retained |
KaMin Polyfil® HG Kaolin Clay - Waterwashed Polyfil® HG is an ultra-fine particle size, moderate brightness water washed kaolin clay. It offers acid resistance, barrier properties, reinforcement, neutral ph, and extremely low crystalline .. |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | 0.005% Retained |
KaMin Polyfil® HG90 Kaolin Clay - Waterwashed High brightness, ultra-fine kaolin extender for white or bright colored rubber or plastic, spray dried bead form.Industry: Rubber & PlasticUses: Non-Black Rubber, Tire, General Rubber Goods, Butyl R.. |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | 0.01% Retained |
KaMin Polyfil® WC-426 Kaolin Clay - Calcined Fine particle size vinyl-functional calcined clay for outstanding wet electricals and long term stability in wire and cable applications.Industry: Rubber & PlasticUses: Non-Black Rubber, General Rub.. |
|||
Particle Mesh Size | <= 325 Mesh | <= 325 Mesh | 0.01% retained |
Silberline 4-Allâ„¢ E2778 The 4-Allâ„¢ series of passivated aluminum pigments is designed for use in waterborne automotive and industrial coatings. In the 4-Allâ„¢ system, the aluminum pigment is passivated using a pr.. |
|||
Particle Mesh Size | <= 325 Mesh | <= 325 Mesh | 0.01% retained |
Silberline Dedusted Flake Series DF-554 Aluminum Flake DF-554 Dedusted Aluminum Flake is manufactured by incorporating a small amount of Teflonâ„¢ with an uncoated aluminum pigment, and then, through further processing, is provided in a dry, non-dust.. |
|||
Particle Mesh Size | <= 325 Mesh | <= 325 Mesh | 0.1% retained |
Silberline EternaBrite® Premier 251 EternaBrite® Premier 251 is a fine, very bright, leafing aluminum pigment with excellent opacity and distinctness of image (D.O.I) for solvent based general industrial coatings. This grade is not.. |
|||
Particle Mesh Size | <= 325 Mesh | <= 325 Mesh | 1% retained |
Silberline Lansford 243 Standard Series Lansford 243 - is a fine, non-leafing aluminum pigment with good opacity for solvent based industrial coatings. This is a very economical grade with cornflake geometry and wide particle size distrib.. |
|||
Particle Mesh Size | <= 325 Mesh | <= 325 Mesh | 1% retained |
Silberline SilBerCote® 1703-20Z SilBerCote® Z polymer treated aluminum pigments are resistant to acid and alkali staining, while providing enhanced electrical charge resistance in finished coatings. Product is typically formula.. |
|||
Particle Mesh Size | <= 325 Mesh | <= 325 Mesh | 1% retained |
Silberline SilBerCote® 353-20Z SilBerCote® Z polymer treated aluminum pigments are resistant to acid and alkali staining, while providing enhanced electrical charge resistance in finished coatings. Product is typically formula.. |
|||
Particle Mesh Size | <= 325 Mesh | <= 325 Mesh | 0.1% retained |
Silberline SilBerCote® PC 6222X SilBerCote® PC X can be formulated into post-blend and bonded metallic powder coatings. The inorganic surface treatment on the flake imparts improved chemical and environmental resistance propert.. |
|||
Particle Mesh Size | <= 325 Mesh | <= 325 Mesh | 0.01% retained |
Silberline Sparkle Silver® Premier 404AR Sparkle Silver® Premier flakes provide more uniform surfaces than Sparkle Silver® products, and also sharper edges and controlled particle size distribution. "Sparkle Silver® Premier or Sil.. |
|||
Particle Mesh Size | <= 325 Mesh | <= 325 Mesh | 1% retained |
Silberline Sparkle Silver® 3130-AR Sparkle Silver® 3130-AR is a coarse, non-leafing, acid stain resistant aluminum flake pigment with greater hiding power than the related Sparkle Silver® 3122-AR. It is characterized by high sp.. |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | 84% Passes |
Excalibar ExCal® CW 200 Calcium Carbonate CaCO3 Powder ExCal® CW calcium carbonate products are processed from a high-purity ore, to exacting specifications at the Houston, Texas plant. These grades are processed for use in plastics, rubber, coatings,.. |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | 97% Passes |
Excalibar ExCal® CW 325 Calcium Carbonate CaCO3 Powder ExCal® CW calcium carbonate products are processed from a high-purity ore, to exacting specifications at the Houston, Texas plant. These grades are processed for use in plastics, rubber, coatings,.. |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | 8.0% retained |
CIMBAR BARIMITE™ 200 High Purity Barite (BaSO4) Barimite Products are natural, off-white barites produced in Cartersville, Georgia. Cimbar's broad range of Barimite products are clean, high purity, high specific gravity, low solubility and chemi.. |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | 0.0% retained |
CIMBAR CIMBAR™ EX Barite Powder (BaSO4) CIMBAR barite products are made using only the highest quality white, natural barium sulfate ore. CIMBAR barites unique properties of fine grind, high specific gravity, low solubility and chemical .. |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | 0.1% retained |
CIMBAR CIMTUFF® 9107 Talc CIMTUFF® 9100 Series talcs are produced from high purity ore, which provides low iron content, low surface area and excellent color in dry form as well as when incorporated with resins. CIMTUFF® .. |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | 99.0% passing, wet |
CIMBAR Crescent 12 Calcium Carbonate (CaCO3), Fine Powder CIMBAR's Crescent product line is a natural calcium carbonate ground to various particle size distributions. The crystalline structure of the calcium carbonate in Crescent products has a predominan.. |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | 99.5% passing |
CIMBAR Miti-Wite B10 Chemically Purified White Barite (BaSO4) Miti-Wite barite products are produced using a proprietary chemical process to enhance the purity of the natural barium sulfate ore. Miti-Wite products are available in a variety of particle sizes .. |
|||
Particle Mesh Size | 325 Mesh | 325 Mesh | 0.95 |
ATI Wah Chang Reactor Grade Zirconium Oxide, ZrO2 Reactor Grade. A white, free-flowing powder.Information provided by ATI Wah ChangTypical Analysis: On Zr metal basis |