Material Notes:
Transparent sparkling glass-like appearance. Suitable for films, sheets, blow molding, foams and injection molding. It can be used as a polystyrene alternative for heat resistant thin wall containers, a polycarbonate alternative for durable “dishwasher proof” transparent products, and a glass alternative for hot-fill food containers. Information provided by Perstorp Compounds Inc.
Physical Properties Metric English Comments
Specific Gravity 1.27 g/cc
1.27 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Tensile Strength 56.0 MPa
8120 psi
Elongation at Break 140 %
140 %
ASTM D638
Flexural Yield Strength 90.0 MPa
13100 psi
ASTM D790
Flexural Modulus 2.50 GPa
363 ksi
ASTM D790
Izod Impact, Notched 0.240 J/cm
0.450 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Glass Transition Temp, Tg 100 °C
212 °F
ASTM D7426
Optical Properties Metric English Comments
Haze 1.0 %
1.0 %
ASTM D1003
Transmission, Visible 91 %
91 %
ASTM D1003