Phenolic 46%, Carbon fabric 54%

Category Polymer , Thermoset , Carbon Fiber/Thermoset Composite , Phenolic , Phenolic, Carbon Fiber Composite
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Phenolic 46%, Carbon fabric 54%.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Phenolic - Monsanto "SC 1008". Carbon fabric - "VCA"
Physical Properties Metric English Comments
Density 1.36 g/cc
0.0491 lb/in³
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 49.99 MPa
7250 psi
Flexural Yield Strength 102 MPa
14800 psi
Flexural Modulus 6.96 GPa
1010 ksi
Compressive Yield Strength 187 MPa
27100 psi
Compressive Modulus 8.41 GPa
1220 ksi