Polymer Property : Compressive Yield Strength = 187 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Yield Strength 187 MPa
27100 psi
ASTM D695
Sumitomo Bakelite North America 52-40-40-P Long-Glass Reinforced Diallyl Phthalate
Ortho Resin Isomer (DAP). Used for critical, high-performance military and commercial electrical components where long-term reliability is demanded.Meets the requirements of ASTM D5948 Type GDI-30F..
Compressive Yield Strength 187 MPa
27100 psi
Phenolic 46%, Carbon fabric 54%
Phenolic - Monsanto "SC 1008". Carbon fabric - "VCA"