Material Notes:
COPYLENE® CM015G is low melt flow impact copolymer with a barefoot additive package and is designed for excellent processing in injection molding and extrusion applications.Applications:Injection Molding and Extrusion Processes, Film, SheetInformation provided by Phillips 66.
Physical Properties Metric English Comments
Density 0.902 g/cc
0.0326 lb/in³
ASTM D792
Melt Flow 1.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
1.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 23.8 MPa
3450 psi
(2 in/min); ASTM D638
Elongation at Yield 10 %
10 %
ASTM D638
Flexural Modulus 1.07 GPa
155 ksi
0.05 in/mm, 1% Secant, Procedure A; ASTM D790
Izod Impact, Notched NB
NB
Method A; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 77.0 °C
171 °F
Unannealed; ASTM D648
Descriptive Properties Value Comments
Process Extrusion
Film
Injection Molding
Region Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution