Phillips 66 COPYLENE® CR120LN Polypropylene, Random Copolymer, Nucleated

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene Copolymer
Manufacturer Phillips 66
Trade Name COPYLENE®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Phillips 66 COPYLENE® CR120LN Polypropylene, Random Copolymer, Nucleated.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
COPYLENE™ CR120LN is a random copolymer nucleated and with antistat for good mold release in injection molding applications. Applications: Containers, Closures, HousewaresInformation provided by Phillips 66.
Physical Properties Metric English Comments
Density 0.902 g/cc
0.0326 lb/in³
ASTM D792
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 28.3 MPa
4100 psi
2 in/min; ASTM D638
Elongation at Yield 12.2 %
12.2 %
ASTM D638
Flexural Modulus 1.10 GPa
160 ksi
0.05 in/min; 1% secant; Procedure A; ASTM D790
Izod Impact, Notched 0.641 J/cm

@Temperature 23.0 °C
1.20 ft-lb/in

@Temperature 73.4 °F
Method A; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 94.0 °C
201 °F
unannealed; ASTM D648
Descriptive Properties Value Comments
Process Injection Molding
Region Mexico
Bamberger Polymers Distribution
US & Canada
Bamberger Polymers Distribution
Users viewing this material also viewed the following:
Copyright © lookpolymers.com All Rights Reserved