Material Notes:
Characteristics:"Stacked fiber" microstructureExtremely creep resistantApplications:Furnace components - wires, including stranded; sintering and annealing boats; evaporator coilsLighting - retaining and feed wiresInformation provided by Plansee.
Physical Properties Metric English Comments
Specific Gravity 10.2 g/cc
10.2 g/cc
Calculated
Thermal Properties Metric English Comments
Thermal Conductivity 142 W/m-K
985 BTU-in/hr-ft²-°F
comparable with pure Mo
Maximum Service Temperature, Air 2000 °C
3630 °F
Microstructure stable up to this point
Component Elements Properties Metric English Comments
Molybdenum, Mo 99.3 %
99.3 %
Balance
Other, each 0.70 %
0.70 %
Lanthanum Oxide
Descriptive Properties Value Comments
Creep Resistance < 1400°C
much greater than pure Mo
Ductility much greater than pure Mo
after HT use
Recrystallization Temperature much greater than pure Mo
Stability at High Temperature > 1400°C
greater than pure Mo
Stability at Room Temperature comparable with pure Mo
Weldability greater than pure Mo