Plaskolite Duraplex® SG-10 Sign Grade Acrylic Sheet, Impact Modified

Category Polymer , Thermoplastic , Acrylic (PMMA) , Acrylic, Optical Sheet
Manufacturer Plaskolite
Trade Name Duraplex®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plaskolite Duraplex® SG-10 Sign Grade Acrylic Sheet, Impact Modified.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Available in unlimited lengths - no seams in finished products.Data provided by the manufacturer, Plaskolite, Inc.
Physical Properties Metric English Comments
Density 1.15 g/cc
0.0415 lb/in³
ASTM D792
Water Absorption 0.30 %
0.30 %
ASTM D570
Linear Mold Shrinkage 0.0030 - 0.0060 cm/cm
0.0030 - 0.0060 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell M 46
46
Method A; ASTM D785
Tensile Strength, Yield 39.0 MPa
5660 psi
ASTM D638
Tensile Modulus 1.70 GPa
247 ksi
ASTM D638
Flexural Yield Strength 57.0 MPa
8270 psi
ASTM D790
Izod Impact, Notched 1.10 J/cm
2.06 ft-lb/in
ASTM D256
0.500 J/cm

@Temperature -18.0 °C
0.937 ft-lb/in

@Temperature -0.400 °F
ASTM D256
Gardner Impact 5.30 J
3.91 ft-lb
reported as J/cm; ASTM D3029-GB, unpainted
Thermal Properties Metric English Comments
CTE, linear 90.0 µm/m-°C

@Temperature -18.0 - 38.0 °C
50.0 µin/in-°F

@Temperature -0.400 - 100 °F
ASTM D696
Deflection Temperature at 1.8 MPa (264 psi) 82.0 °C
180 °F
annealed; ASTM D648
Optical Properties Metric English Comments
Haze 3.0 %
3.0 %
ASTM D1003
Transmission, Visible 90 %
90 %
ASTM D1003
Processing Properties Metric English Comments
Processing Temperature 154 °C
309 °F
Optimal Thermoforming temperature for sheet 0.25-1.0 cm (0.10-0.39 in)