Plaskolite Optix® CA-945 Clear Impact Modified Acrylic Resin

Category Polymer , Thermoplastic , Acrylic (PMMA) , Acrylic, Extruded
Manufacturer Plaskolite
Trade Name Optix®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plaskolite Optix® CA-945 Clear Impact Modified Acrylic Resin.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Impact modified acrylic resin, extrusion and injection moldingApplications: An impact-modified acrylic resin for extrusion and injection molding. This resin offers impact strengths up to six times of general-purpose acrylic resins. It also offers good heat resistance.
Physical Properties Metric English Comments
Density 1.17 g/cc
0.0423 lb/in³
ASTM D792
Melt Flow 1.7 g/10 min
1.7 g/10 min
ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 55.2 MPa
8010 psi
ASTM D638
Elongation at Break 25 %
25 %
ASTM D638
Izod Impact, Notched 0.430 J/cm
0.806 ft-lb/in
ASTM D256
Gardner Impact 2.60 J
1.92 ft-lb
Falling Weight; ASTM D3029GB
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 88.0 °C
190 °F
ASTM D648
Optical Properties Metric English Comments
Transmission, Visible 91.6 %
91.6 %
ASTM D1003