Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plastics Group Polifil® 78MRGF Glass Fiber and Mineral Reinforced Nylon 6/6 (DAM)

Category Polymer , Thermoplastic , Nylon , Nylon 66 , Nylon 66, Glass/Mineral Filled
Manufacturer The Plastics Group of America
Trade Name Polifil®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastics Group Polifil® 78MRGF Glass Fiber and Mineral Reinforced Nylon 6/6 (DAM).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polifil® GFN/MRN 6/6 reinforced series of compounds offer superior strength, rigidity and creep resistance. Glass fibers provide excellent thermal and dimensional stability while maintaining good heat and chemical resistance.Applications: Bike componentsFuel capsAutomotive componentsStandard processing techniques are applicable.Information provided by The Plastics Group.
Physical Properties Metric English Comments
Density 1.45 g/cc
0.0524 lb/in³
ASTM D792
Water Absorption 0.70 %
0.70 %
24 hours; ASTM D570
Linear Mold Shrinkage 0.0050 cm/cm

@Thickness 3.17 mm
0.0050 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength at Break 85.5 MPa
12400 psi
ASTM D638
Elongation at Break 12 %
12 %
ASTM D638
Flexural Modulus 4.07 GPa
590 ksi
Tangent; ASTM D790
Izod Impact, Notched 0.641 J/cm
1.20 ft-lb/in
At 73°F; ASTM D256
Thermal Properties Metric English Comments
Melting Point 260 °C
500 °F
ASTM D789
Deflection Temperature at 0.46 MPa (66 psi) 257 °C
495 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 235 °C
455 °F
ASTM D648