Plastics Group Polifil® GFPC-10 10% Glass-Reinforced Polycarbonate

Category Polymer , Thermoplastic , Polycarbonate (PC) , Polycarbonate, 10% Glass Filled
Manufacturer The Plastics Group of America
Trade Name Polifil®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastics Group Polifil® GFPC-10 10% Glass-Reinforced Polycarbonate.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polifil® GFPC series compounds offer a combination of improved dimensional stability and decreased flammability. The excellent balance of physical properties make the Polifil® glass-filled polycarbonate line an excellent choice for electrical, appliance and hardware applications. Standard processing techniques are applicable. Information provided by The Plastics Group.
Physical Properties Metric English Comments
Density 1.26 g/cc
0.0455 lb/in³
ASTM D792
Filler Content 10 %
10 %
ASTM D2584
Linear Mold Shrinkage 0.0020 - 0.0040 cm/cm

@Thickness 1.59 mm
0.0020 - 0.0040 in/in

@Thickness 0.0625 in
ASTM D955
Melt Flow 12 - 20 g/10 min
12 - 20 g/10 min
300/1.2; May be specified; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 121
121
ASTM D785
Tensile Strength at Break 66.2 MPa
9600 psi
ASTM D638
Elongation at Break 12 %
12 %
ASTM D638
Tensile Modulus 2.86 GPa
415 ksi
ASTM D790
Flexural Strength 101 MPa
14700 psi
ASTM D790
Flexural Modulus 3.93 GPa
570 ksi
Tangent; ASTM D790
Izod Impact, Notched 1.07 J/cm
2.00 ft-lb/in
At 73°F; ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 135 °C
275 °F
ASTM D648
Flammability, UL94 HB
HB