Physical Properties | Metric | English | Comments |
---|---|---|---|
Density | 1.26 g/cc | 0.0455 lb/in³ | ISO 1183 |
Nilit FRIANYL B63 KV20 Nylon 6 for injection molding, 20% glass ball reinforced Nylon 6 for injection molding.Information provided by Frisetta Polymer, which merged into Nilit Plastics |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® EXL5689 PC Copolymer (Asia Pacific) Lexan* EXL5689 polycarbonate (PC) resin is a GF reinforced, UV stabilized, flame retardant injection molding copolymer blend. This medium flow resin features UL94 V0 @ 1.5mm flame retardancy based .. |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® ML7667 PC Copolymer (Europe-Africa-Middle East) Lexan* ML7667 specialty polycarbonate (PC) resin is a 9% GF reinforced, UV stabilized, flame retarded injection molding grade. This medium flow specialty PC resin combines UL94 V0 @ 1.5mm, 5VB @ 3.. |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | ASTM D1475 |
BASF Master Builders Solutions ChemRex® CX-943 Squeegee-grade Polyurethane Adhesive
(discontinued **) CX-943 is a one-component polyurethane-based squeegee-grade, structural adhesive. Its elastomeric properties enable it to move with substrates as it expands and contracts. The patented formula is .. |
|||
Density | 1.26 - 1.65 g/cc | 0.0454 - 0.0596 lb/in³ | Average value: 1.33 g/cc Grade Count:74 |
Overview of materials for Polyetheretherketone, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyetheretherketone, Unreinforced". Each property range of values reported is minimum and maximum value.. |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | ASTM D792 |
Solvay Specialty Polymers Amodel® A-1115 HS Polyphthalamide (PPA) Resin, 15% Glass Reinforced, Dry As Molded
AMODEL A-1115 HS resin is a 15% glass reinforced, heat stabilized polyphthalamide (PPA) which exhibits a high deflection temperature, high flexural modulus, and high tensile strength. Excellent cre.. |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | Amorphous; ISO 1183 |
Victrex® PEEK 600G Polyetheretherketone
(discontinued **) Product Description: High performance thermoplastic material, unreinforced PolyEtherEtherKetone (PEEK), semi crystalline, granules for injection moulding and extrusion, low viscosity, FDA food conta.. |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | ASTM D792B |
LyondellBasell Astryn 75F4-4 Polypropylene Copolymer, 40% Talc Key Features: conventional melt flow, high modulus, mineral-filled polypropylene copolymer, high strength, high stiffness, good aestheticsApplications: small appliances, electrical components, house.. |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | |
LATI Latilub 66-20ST PA66, Silicone/PTFE Filled Self-lubricating product based on Polyamide 66 (PA66). Silicone / PTFE. Availability: Africa & Middle East; Asia Pacific; Europe; Latin America; North AmericaInformation provided by Lati Industria T.. |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | |
Solvay Chemicals CASO® TEC SOLUTION 25-29% Calcium Chloride CASO® Calcium Chloride technical grade can be used in various applications in industrial, public and private sectors.REACH Registration Number: 01-2119494219-28/ CAS number: 10043-52-4/ EINECS - .. |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | ISO 1183 |
Solvay Specialty Polymers Amodel® A-1625 HS Polyphthalamide (PPA), 25% GlassCarbon Fiber Amodel® A-1625 HS is a 25% carbon and glass-reinforced, heat-stabilized grade of polyphthalamide (PPA). It is formulated for applications requiring the dissipation of static charge. This material.. |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Xenoy® X4820 PBT+PC (Asia Pacific) Xenoy X4820 is a high modulus PC/PBT Blend. This resin provides high chemical resistance, excellent impact, very low creep, low CTE, excellent fatigue and dimensional stability. |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP NX10302 PC+ABS (Asia Pacific) This is a PC/ABS compound with improved plating, surface and mechanical performance, a good candidate for Laser Direct Structuring applications. |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | ASTM D792 |
SABIC Innovative Plastics LNP THERMOCOMP RF003ES PA 66 LNP* THERMOCOMP* RF003ES is a Nylon 66 base resin containing 15% Glass Fiber. Added features of this material include: Easy Molding, Heat Stabilized. |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | ISO 1183 |
SABIC Innovative Plastics LNP STAT-KON DE003E PC (Europe-Africa-Middle East) LNP* Stat-kon* DE003E is a compound based on Polycarbonate resin containing Carbon Fiber. Added features of this material include: Easy Molding, Electrically Conductive. |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | ISO 1183 |
Unitika A175G15 PA66, 15% Glass Fiber Reinforced, Dry Information provided by Unitika Ltd. |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | DIN 53479 |
Polyram PlusTek PB350M4 Nylon 6, 20% Mineral Filled 20% mineral filled polyamide 6 for injection molding applicationsInformation provided by Polyram Ram On Ind. |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | Cured resin density |
Hexcel® HexPly® 1454 125°C Curing Epoxy Matrix HexPly® 1454 is a self-extinguishing epoxy resin system with very high self adhesion properties. It has good handling and is tolerant of a wide range of processing conditions. HexPly® 1454 is idea.. |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | JIS-Z-8807 |
Denka REOMER G G3070 Thermoplastic Elastomer, For Extrusion Essentially a thermoplastic elastomer with the characteristics of PVC resin and rubber, with excellent rubber-like elasticity. Offers excellent rubbery characteristics, such as permanent compressive.. |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | JIS-Z-8807 |
Denka REOMER G G5074 Thermoplastic Elastomer, For Extrusion Essentially a thermoplastic elastomer with the characteristics of PVC resin and rubber, with excellent rubber-like elasticity. Offers excellent rubbery characteristics, such as permanent compressive.. |
|||
Density | 1.26 - 1.30 g/cc | 0.0455 - 0.0470 lb/in³ | ISO R 1183 |
Fainplast Compounds FR 008 Flexible PVC, Insulation Insulation |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | ASTM D792 |
Aclo Accutech ABS ABS831G30L Glass Reinforced |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | ASTM D792 |
Adell BJ-14 Nylon 6, 20% Glass Reinforced; High Impact Data provided by Adell Plastics, Inc. |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | |
Arlon CP-310R Bulk Compound Appearance: Red silicone gumThis data represents typical values for the production material. The data should not be used to write, or in place of, material specifications.Information provided by Arl.. |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | |
A. Schulman ComAlloy Hiloy® 223 ABS, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | ASTM D792 |
Aclo Accutech Polycarbonate POL050G10L Glass Reinforced |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | |
A. Schulman ComAlloy Hiloy® 249 SAN, Glass Reinforced Data provided by the manufacturer, ComAlloy International Company.30% Glass Reinforced.The ComAlloy product line has been integrated into the A Schulman product line. |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | ASTM D792 |
Teknor Apex Sarlink® 4339D Thermoplastic Elastomer A highly engineered thermoplastic elastomer for use in demanding applications. Sarlink® 4339D is a flame retardant, high hardness grade processing exceptional chemical resistance, compression set .. |
|||
Density | 1.26 g/cc | 0.0455 lb/in³ | ISO 1183 |
SABIC Innovative Plastics Lexan® EXL5689 PC Copolymer Lexan* EXL5689 polycarbonate (PC) resin is a GF reinforced, UV stabilized, flame retardant injection molding copolymer blend. This medium flow resin features UL94 V0 @ 1.5mm flame retardancy based .. |
|||
Density | 1.26 - 1.65 g/cc | 0.0455 - 0.0596 lb/in³ | Average value: 1.48 g/cc Grade Count:12 |
Overview of materials for Polyphthalamide (PPA), 10% Glass Fiber Reinforced This property data is a summary of similar materials in the MatWeb database for the category "Polyphthalamide, 10% Glass Fiber Reinforced". Specific grades with glass content between 5% and 14% are .. |