Plastics Group Polifil® GFPP-40 40% Glass-Reinforced Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene with 40% Glass Fiber Filler
Manufacturer The Plastics Group of America
Trade Name Polifil®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastics Group Polifil® GFPP-40 40% Glass-Reinforced Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polifil® GFPP series compounds are homopolymer polypropylene resins reinforced with glass fibers. They provide high impact with increased strength, stiffness, surface hardness, and higher continuous temperature. Other benefits include reduced distortion under long-term stress.Applications: AppliancesElectrical componentsAutomotiveUtility productsStandard processing techniques are applicable. Information provided by The Plastics Group.
Physical Properties Metric English Comments
Density 1.22 g/cc
0.0441 lb/in³
ASTM D792
Filler Content 40 %
40 %
ASTM D2584
Linear Mold Shrinkage 0.0020 cm/cm

@Thickness 1.59 mm
0.0020 in/in

@Thickness 0.0625 in
ASTM D955
Melt Flow 8.0 - 12 g/10 min
8.0 - 12 g/10 min
230/2.16; May be specified; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength at Break 53.8 MPa
7800 psi
ASTM D638
Flexural Strength 78.6 MPa
11400 psi
ASTM D638
Flexural Modulus 5.52 GPa
800 ksi
Tangent; ASTM D790
Izod Impact, Notched 0.641 J/cm
1.20 ft-lb/in
At 73°F; ASTM D256
Gardner Impact 0.305 J
0.225 ft-lb
ASTM D3029
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 146 °C
294 °F
ASTM D648