Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Plastics Group Polifil® RP-PP Polypropylene, Black

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer The Plastics Group of America
Trade Name Polifil®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plastics Group Polifil® RP-PP Polypropylene, Black.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Polifil® RP-PP reprocessed polypropylene has the highest stiffness of the commodity olefin resins, while retaining sufficient impact properties for many applications. Due to its low cost and low density, polypropylene use has been expanding rapidly, and common uses now include injection molded articles, fibers, packaging films, and extruded sheet and profiles. Polypropylene is widely used in injection molding for housewares, appliances, and automotive parts. High flow grades are spun into fibers, and molded into thin wall containers, cups, and lids. Moderate flow resins are common in general injection molding and cast films. High molecular weight, low flow grades are extruded into sheet and profiles, and blow molded into automotive parts and recreational goods.Information provided by The Plastics Group.
Physical Properties Metric English Comments
Density 0.905 g/cc
0.0327 lb/in³
ASTM D792
Water Absorption 0.00 %
0.00 %
24 hours; ASTM D570
Melt Flow 12 g/10 min
12 g/10 min
230/2.16, nominal; ASTM D1238
Mechanical Properties Metric English Comments
Tensile Strength, Yield 25.5 MPa
3700 psi
ASTM D638
Elongation at Break >= 200 %
>= 200 %
ASTM D638
Flexural Modulus 1.10 GPa
160 ksi
1% Secant; ASTM D790
Izod Impact, Notched 0.427 J/cm
0.800 ft-lb/in
ASTM D256
Izod Impact, Unnotched NB
NB
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 86.7 °C
188 °F
ASTM D648
Users viewing this material also viewed the following: