Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 86.7 °C
188 °F
ASTM D648
RheTech Products FT4650-00 Thermoplastic Polyolefin, Non-UV Stabilized, Natural
Applications: Scuff platesExterior grillesBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 0.46 MPa (66 psi) 86.7 °C
188 °F
ASTM D648
RheTech Products FT4650-581UV Thermoplastic Polyolefin, UV Stabilized, HD2 Medium Quartz Metallic
Applications: Scuff platesExterior grillesBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 0.46 MPa (66 psi) 86.7 °C
188 °F
ASTM D648
RheTech Products FT4650-583UV Thermoplastic Polyolefin, UV Stabilized, Exterior DX9 Black
Applications: Scuff platesExterior grillesBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products.
Deflection Temperature at 0.46 MPa (66 psi) 86.7 °C
188 °F
ASTM D648
Ineos H02G-02 Polypropylene Homopolymer
This is a homopolymer designed for extrusion and film. It exhibits good extrusion and film orientation behavior. This material meets the requirements of the U.S. Food and Drug Administration as sp..
Deflection Temperature at 0.46 MPa (66 psi) 86.7 °C
188 °F
ASTM D648
Ineos N00G-01 Polypropylene Impact Copolymer
Grade N00G-01 is a fractional melt flow rate impact copolymer for blow molding, pipe, tubing, and sheet extrusion. It offers a good balance of stiffness and impact strength as compared to other impa..
Deflection Temperature at 0.46 MPa (66 psi) 86.7 °C
188 °F
ASTM D648
Ineos N20L-00 Polypropylene Impact Copolymer
This is a nucleated polypropylene impact copolymer formulated with a slip agent for improved mold release, and has an optimum balance of stiffness and impact resistance for injection molding applica..
Deflection Temperature at 0.46 MPa (66 psi) 86.7 °C
188 °F
Unannealed; ASTM D648
Techmer ES HiFill FR® PP CO FR-N V2
Availability: North AmericaForms: PelletsFeatures: Flame Retardant, High Impact Resistance and CopolymerInformation provided by TP Composites, Inc.
Deflection Temperature at 0.46 MPa (66 psi) 86.7 °C
188 °F
ASTM D648
Plastics Group Polifil® RP-PP Polypropylene, Black
Polifil® RP-PP reprocessed polypropylene has the highest stiffness of the commodity olefin resins, while retaining sufficient impact properties for many applications. Due to its low cost and low de..