Plenco 7321 Phenolic, Granular, Transfer Molded

Category Polymer , Thermoset , Filled/Reinforced Thermoset , Phenolic
Manufacturer Plenco (Plastics Engineering Company)
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Plenco 7321 Phenolic, Granular, Transfer Molded.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
PLENCO 07321 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength and excellent dimensional stability. Type ASTM 5948 CFI-5, and UL recognized under component file E40654. 07321 is available in black.Information supplied by Plenco.
Physical Properties Metric English Comments
Bulk Density 0.470 g/cc
0.0170 lb/in³
ASTM D1895
Density 1.40 g/cc
0.0506 lb/in³
ASTM D792
Water Absorption 0.37 %
0.37 %
ASTM D570
Linear Mold Shrinkage 0.0091 cm/cm
0.0091 in/in
ASTM D955
Mechanical Properties Metric English Comments
Hardness, Rockwell E 76
76
ASTM D785
Tensile Strength, Ultimate 43.0 MPa
6240 psi
ASTM D638
Elongation at Break 0.71 %
0.71 %
ASTM D638
Tensile Modulus 6.90 GPa
1000 ksi
ASTM D638
Flexural Strength 67.0 MPa
9720 psi
ASTM D790
Flexural Modulus 6.70 GPa
972 ksi
ASTM D790
Compressive Strength 179 MPa
26000 psi
ASTM D695
Izod Impact, Notched 0.284 J/cm
0.532 ft-lb/in
ASTM D256
Charpy Impact, Notched 0.291 J/cm²
1.38 ft-lb/in²
ASTM D256
Impact 310
310
J/m Drop Ball Impact; PLENCO
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 187 °C
369 °F
Heat Resistance; ASTM D570D
Deflection Temperature at 1.8 MPa (264 psi) 163 °C
325 °F
ASTM D648
Flammability, UL94 HB

@Thickness 1.50 mm
HB

@Thickness 0.0591 in
Shrinkage 0.29 %
0.29 %
72 hr, 120ºC; ASTM D1299
Electrical Properties Metric English Comments
Volume Resistivity 1.70e+11 ohm-cm
1.70e+11 ohm-cm
ASTM D247
Dielectric Constant 5.3
5.3
ASTM D150
Dielectric Strength 8.30 kV/mm
211 kV/in
Short Time; ASTM D149
Dissipation Factor 0.074
0.074
ASTM D150
Arc Resistance 133 sec
133 sec
ASTM D495
Comparative Tracking Index 150 V
150 V
ASTM D3638