Polymer Property : Compressive Strength = 179 MPa Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Compressive Strength 179 MPa
26000 psi
Compression after impact strength, 1500 in-lb/in; NASA 1092
Park Electrochemical Nelcote® V-376 Cyanate Ester Epoxy Prepregs, 581 Quartz Reinforced
Nelcote® V-376 is a Cyanate Ester matrix providing excellent electrical and mechanical properties for harsh aircraft, shipboard, and undersea applications for Radomes, Antenna, and Reflectors. Simp..
Compressive Strength 179 MPa
26000 psi
ASTM D695
Quantum PEEK 30% Glass Fiber Filled
Information provided by Quantum Advanced Engineering Plastics
Compressive Strength 179 MPa
26000 psi
ASTM D695
Resinoid 2215 Phenolic Molding, Cellulose Reinforced
Data provided by the manufacturer.The Resinoid 2000 organic fiber reinforced series compounds feature mechanical strength, dimensional stability, and shock resistance
Compressive Strength 179 MPa
26000 psi
ASTM D695
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Typical applications include ..
Compressive Strength 179 MPa
26000 psi
ASTM D695
Technetics Group Amicon™ PEEK 30% Glass Filled  (Unverified Data**)
Information provided by Technetics Group (formerly Plastomer Technologies)
Compressive Strength 179 MPa
26000 psi
10% Def.; ASTM D695
Quadrant EPP Semitron® ESd 490HR Static dissipative PEEK for use in test fixtures. Non-sloughing and low moisture absorption. (ASTM Product Data Sheet)
Compressive Strength 179 MPa
26000 psi
ASTM D695
PolyOne Edgetek® SF-47GF/000 Polyphenylene Sulfide (PPS), Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
Compressive Strength 179 MPa
26000 psi
ASTM D695
IDI Composites 46-16 Thermoset Polyester, Molding
Premium high strength electrical grade with excellent resistance to smoke generation, weathering, and corrosive environments.Data provided by the manufacturer.
Compressive Strength 179 MPa
26000 psi
SGL Carbon Group EK 24 Carbon Graphite
Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and..
Compressive Strength 179 MPa
26000 psi
ASTM D695
Solvay Specialty Polymers Amodel® A-4133 HH Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® A-4133 HH is a 33% glass fiber reinforced heat stabilized grade of polyphthalamide (PPA) that has been designed to provide outstanding property retention to thermal oxidative degradation ..
Compressive Strength 179 MPa
26000 psi
ASTM D695
Solvay Specialty Polymers Amodel® A-4145 HH Polyphthalamide (PPA), 45% Glass Fiber (Dry)
Amodel® A-4145 HH is a 45% glass fiber reinforced heat stabilized grade of polyphthalamide (PPA) that has been designed to provide outstanding property retention to thermal oxidative degradation ..
Compressive Strength 179 MPa
26000 psi
ASTM D695
Solvay Specialty Polymers Amodel® AS-4133 HS Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® AS-4133 HS is a 33% glass reinforced, lubricated, heat stabilized grade of polyphthalamide (PPA) that offers fast cycle times and moldability in hot water molds. Testing conducted on samp..
Compressive Strength 179 MPa
26000 psi
ASTM D695
Solvay Specialty Polymers Amodel® AS-4133 L Polyphthalamide (PPA), 33% Glass Fiber (Dry)
Amodel® AS-4133 L polyphthalamide (PPA) a 33% glass reinforced, lubricated, structural grade of polyphthalamide (PPA) that offers fast cycle times and is hot water moldable. Typical applications ..
Compressive Strength 179 MPa
26000 psi
ASTM D695
Sumitomo Bakelite Durez® 153 Phenolic, Compression Grade
Durez 153 Black Phenolic is a two-stage, asbestos-free, heat resistant/electrical molding material. It exhibits good molded appearance and shock resistance for use on a wide variety of electrical a..
Compressive Strength 179 MPa
26000 psi
ASTM D695
Sumitomo Bakelite Sumikon® PM-6430 Glass-Filled Phenolic, Injection Grade
Sumikon PM-6430 black Phenolic is a two stage glass fiber and mineral filled special purpose molding compound. It is especially designed for applications requiring high strength and dimensional s..
Compressive Strength 179 MPa
26000 psi
Cosmic Plastics K43 Mineral Filled Iso Diallyl Phthalate Molding Compound
Data provided by the manufacturer.
Compressive Strength 179 MPa
26000 psi
ASTM D695
Plenco 7321 Phenolic, Granular, Transfer Molded
PLENCO 07321 is an organic fiber reinforced phenolic molding compound, offering improved mechanical strength and excellent dimensional stability. Type ASTM 5948 CFI-5, and UL recognized under compon..
Compressive Strength 179 MPa
26000 psi
ASTM D695
Plenco 7507 Phenolic, Granular, Transfer Molded
PLENCO 07507 is an organic reinforced phenolic molding compound offering improved dimensional stability under humid conditions. 07507 offers excellent resistance to degradation from detergent solut..
Compressive Strength 179 MPa
26000 psi
10% Deformation; ASTM D695
Ensinger Tecapeek® XP-98 Compression Molded PEEK Compound, 30% Carbon Fiber
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in..
Compressive Strength <= 179 MPa
<= 26000 psi
ASTM D695
Ensinger Tecapeek® XP-98 Medical Compression Molded PEEK Compound, 30% Carbon Fiber
Ensinger Special Polymers offers over twenty different VICTREX® PEEK blends to choose from and has the capability to blend custom compounds for specific applications. Compression molding results in..
Compressive Strength 179 - 214 MPa
26000 - 31000 psi
Bulk Molding Compounds BMC 685 Mineral Filled, Glass Fiber Reinforced Polyester Compound
BMC 685 molding compound is a mineral filled, glass fiber-reinforced polyester compound suitable for compression, transfer and stuffer injection molding It is characterized by good moldability, oil ..
Compressive Strength 179 MPa

@Strain 10.0 %,
Temperature 22.8 °C
26000 psi

@Strain 10.0 %,
Temperature 73.0 °F
ASTM D695
Quadrant EPP Duratron® U2100 OEI Extruded 10% Glass Reinforced Polyetherimide
Compressive Strength 179 MPa
26000 psi
ASTM D695
PolyOne Edgetek® SF-45GF/000 Polyphenylene Sulfide (PPS), Glass Filled  (discontinued **)
Description/Features:Glass Fiber ReinforcedUL 94 V0PolyOne First ChoiceInformation provided by PolyOne Corporation.
Compressive Strength 179 MPa
26000 psi
ASTM D695
Solvay Specialty Polymers Amodel® AS-4133 L Polyphthalamide (PPA)  (Unverified Data**)
Amodel AS-4133 L polyphthalamide (PPA) a 33% glass reinforced, lubricated, structural grade of polyphthalamide (PPA) that offers fast cycle times and is hot water moldable. Typical applications incl..
Compressive Strength 179 MPa
26000 psi
ASTM D695
Solvay Specialty Polymers Amodel® AS-4133 HN Polyphthalamide (PPA), Dry, 33% Glass Fiber Reinforcement, Heat Stabilizer
Amodel AS-4133 HN polyphthalamide (PPA) is a non-lubricated, heat stabilized grade that offers fast cycle times and is hot-water moldable. Typical applications include electrical and electronic comp..