Poco Graphite DFP-3-2 Ion Implant Grade Graphite

Category Carbon , Graphite
Manufacturer Poco Graphite
Trade Name
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Poco Graphite DFP-3-2 Ion Implant Grade Graphite.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
This is a high strength graphite that has reduced porosity. DFP-3-2 has long been the standard for components that exhibit long life and reduced erosion rates.
Physical Properties Metric English Comments
Apparent Bulk Density 1.82 g/cc
0.0658 lb/in³
Particle Size 4.0 µm
4.0 µm
Mechanical Properties Metric English Comments
Hardness, Shore D 74
74
Flexural Strength 82.7 MPa
12000 psi
Compressive Strength 138 MPa
20000 psi
Thermal Properties Metric English Comments
CTE, linear 8.10 µm/m-°C
4.50 µin/in-°F
Electrical Properties Metric English Comments
Electrical Resistivity 0.00152 ohm-cm
0.00152 ohm-cm
Descriptive Properties Value Comments
Purity 0.999995