Polimeri Europa Europrene® SOL T 9133 Styrene - Isoprene Block Copolymer

Category Polymer , Thermoplastic , Elastomer, TPE , Styrenic TPE
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Europrene®
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Europrene® SOL T 9133 Styrene - Isoprene Block Copolymer.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Europrene® SOL T 9133 is a linear block copolymer obtained by anionic polymerization. The polymer is based on styrene and isoprene, where bound styrene content is 16% weight and diblock content is 55%. A non-staining, TNPP free antioxidant system is added during the production process.Key Features: Europrene® SOL T 9133 is a block copolymer with linear molecular structure and very high diblock content, designed for hot melt pressure sensitive applications where excellent tack performance, combined with softness and low viscosity, are required.Main Applications: Hot melt pressure-sensitive adhesive for labels or high tack tapes.Information provided by Polimeri Europa. Mechanical properties measured on ASTM D 4703 compression molded samples.
Physical Properties Metric English Comments
Specific Gravity 0.920 g/cc
0.920 g/cc
ASTM D792
Brookfield Viscosity 0.060 cP
0.060 cP
Toluene sol., 25% wt; ASTM D1084
Melt Flow 14 g/10 min

@Load 5.00 kg,
Temperature 190 °C
14 g/10 min

@Load 11.0 lb,
Temperature 374 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 20
20
ASTM D2240
Tensile Strength at Break 4.00 MPa
580 psi
ASTM D412
Elongation at Break 1300 %
1300 %
ASTM D412
300% Modulus 0.000500 GPa
0.0725 ksi
ASTM D412