Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polimeri Europa Extir® CM Giotto 5 Expandable Polystyrene - Continuous Mass

Category Polymer , Thermoplastic , Polystyrene (PS) , Expanded Polystyrene (EPS)
Manufacturer Polimeri Europa (Former EniChem)
Trade Name Extir®
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa Extir® CM Giotto 5 Expandable Polystyrene - Continuous Mass.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of blowing agent. Extir CM does not contain CFC or HCFC. Extir CM Giotto 5 is a white product with improved thermal conductivity.Applications: Extir CM Giotto 5 has an improved coefficient of thermal insulation. Blocks exhibit good compressive strength and fusion combined with an excellent surface finish after cutting. Typical applications are: low density blocks for thermal insulationcomposite EPS/plasterboard for internal wall insulationlow density flooring slabscut packagingInformation provided by Polimeri Europa.
Physical Properties Metric English Comments
Bulk Density 0.590 - 0.630 g/cc
0.0213 - 0.0228 lb/in³
Density >= 0.0120 g/cc
>= 0.000434 lb/in³
Minimum apparent density on a continuous pre-expander after two expansions
>= 0.0160 g/cc
>= 0.000578 lb/in³
Minimum apparent density on a discontinuous pre-expander
>= 0.0180 g/cc
>= 0.000650 lb/in³
Minimum apparent density on a continuous pre-expander after one expansion
0.0120 - 0.0250 g/cc
0.000434 - 0.000903 lb/in³
Density range normally used
Particle Size 900 - 1600 µm
900 - 1600 µm