Physical Properties | Metric | English | Comments |
---|---|---|---|
Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | Loose |
Nyco NYGLOS® M20 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir® CM Galileo Europa 5 AE Expandable Polystyrene - Continuous Mass Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of .. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir® LN 3000 Expandable Polystyrene Extir LN 3000 belongs to a new expandable product family, the Leonardo Series, with improved processing features: high expandability, high moulding productivity, wide processing area, optimal fusion.. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir® CM Galileo Io 5 AE Expandable Polystyrene - Continuous Mass Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of .. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir® CM Giotto 5 AE Expandable Polystyrene - Continuous Mass/Flame Retardant Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of .. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir® CM Giotto 5 Expandable Polystyrene - Continuous Mass Product Description:Extir CM is the new expandable products range produced with the new Continuous Mass technology. All the products have a very low dimensional dispersion and a reduced content of .. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir® EH 2000 Expandable Polystyrene Extir EH 2000 is an expandable polystyrene in the form of spherical beads of fine particle size, with a low pentane content as blowing agent. Extir does not contain CFC or HCFC. Extir EH 2000 is use.. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir® EH 3000 Expandable Polystyrene Extir EH 3000 is an expandable polystyrene in the form of spherical beads of medium particle size, with a low pentane content as blowing agent. Extir does not contain CFC or HCFC. Extir EH 3000 is u.. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir® GEO 3000 AE Expandable Polystyrene - Flame Retardant Product Description:Extir GEO 3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent.Extir does not contain C.. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir Leonardo A 7000 AE Expandable Polystyrene
(discontinued **) Extir A 7000 AE is a flame retardant expandable polystyrene in the form of spherical beads of large particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Extir A 7.. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir Leonardo B 3000 AE Expandable Polystyrene
(discontinued **) Extir B 3000 AE is a flame retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. This grad.. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir® D 3000 AE Expandable Polystyrene
(discontinued **) Extir D 3000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium particle size, containing pentane as blowing agent. Extir does not contain CFC or CFC. Extir D 30.. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir® E 2000 AE Expandable Polystyrene
(discontinued **) Extir E 2000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of fine particle size, with a low pentane content as blowing agent. Extir does not contain CFC or HCFC. Thi.. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir® F 1111 Expandable Polystyrene
(discontinued **) Extir F 1111 is an expandable polystyrene in the form of spherical beads of very fine particle size and a narrow particle size distribution, containing pentane as blowing agent. Extir does not cont.. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir® P 1212 Expandable Polystyrene
(discontinued **) Extir P 1212 is an expandable polystyrene in the form of spherical beads of very fine particle size and narrow distribution, containing pentane as blowing agent. Extir does not contain CFC or HCFC. .. |
|||
Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | ASTM D1895 |
Chevron Phillips HiD® 94312 HDPE Extrusion Coating Resin
(discontinued **) Resin Type: Melt blend, FDA approvedCharacteristics: Good processabilityGood drawdown capabilityImproved MVTR propertiesGrease resistanceApplications: MVTR applicationsRelease linersCup stockInforma.. |
|||
Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | |
SGL Carbon Group CF 270 Graphite Filler Good mechanical strength, good sliding properties, high temperature resistance, high thermal shock resistance, low wettability, high corrosion resistance, high thermal conductivity, high purity, and.. |
|||
Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | |
Silon TA 2347 HD Orange Catalyst Masterbatch Masterbatch for use with SILON Silane cross-linkable PE-Xb Compounds TA 1108 HD.TA 2347 HD, together with the above mentioned graft, contains the cross-linking catalyst to complete a Sioplas System... |
|||
Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | |
Silon Taborex TA 2329 HD Catalyst Masterbatch Masterbatch for the use with SILON Silane crosslinkable PE-Xb Compounds TA 1117 HD. TA 2329 HD contains a cross-linking catalyst and a stabiliser package. Together with the above-mentioned grafted P.. |
|||
Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | |
Silon Taborex TA 2330 HD Catalyst Masterbatch Masterbatch for the use with SILON Silane crosslinkable PE-Xb Compounds TABOREX TA 1117 HD. TA 2330 HD contains a cross-linking catalyst and a stabiliser package. Together with the above-mentioned g.. |
|||
Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | ASTM D1895 |
Plenco 2000 Phenolic, Granular, Injection Molded PLENCO 02000 is a versatile general purpose, organic filled phenolic molding compound, offering optimum cure characteristics and an excellent balance of molding properties. UL recognized under compo.. |
|||
Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | ASTM D1895 |
Plenco 2571 Phenolic, Granular, Transfer Molded PLENCO 02571 is a general purpose, organic filled phenolic molding compound offering optimum cure characteristics while maintaining excellent mechanical and electrical properties. UL recognized unde.. |
|||
Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | ASTM D1895 |
Plenco 6527 Phenolic, Granular, Transfer Molded PLENCO 06527 is a woodflour and mineral filled resole phenolic molding compound.Information supplied by Plenco. |
|||
Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | ISO 60 |
Vyncolit Neopreg Kinel® SK80 L8G Glass Fiber Reinforced Molding Compound Epoxy based molding compound long glass fiber reinforced with excellent long term property retention over a wide temperature range and climate conditions. It is particularly suited for over mold.. |
|||
Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | |
Zircar Ceramics IB-100A Alumina Bubble Thin wall aluminum oxide ceramic spheres offered in 2 standard bubble sizes. These low density sintered ceramic bodies are useful in a range of refractory applications with temperatures to 2000°C (.. |
|||
Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | ASTM D1895 |
Plenco 2300 Phenolic, Granular, Transfer Molded PLENCO 02300 is a general purpose organic filled molding compound formulated to offer excellent processability while maintaining mechanical strength values. UL recognized under component file E40654.. |
|||
Bulk Density | 0.590 g/cc | 0.0213 lb/in³ | Loose |
Nyco ULTRAFIBRE® M20 Wollastonite Wollastonite is a naturally occurring white mineral with an acicular (needle-shaped) particle structure. This distinctive particle morphology makes wollastonite an ideal performance mineral for a br.. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir® D 5000 AE Expandable Polystyrene - Flame Retardant Product Description:Extir D 5000 AE is a flame-retardant expandable polystyrene in the form of spherical beads of medium-large particle size, containing pentane as blowing agent.Extir does not conta.. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir® EH 5000 Expandable Polystyrene Extir EH 5000 is an expandable polystyrene in the form of spherical beads of medium-large particle size, with a low pentane content as blowing agent. Extir does not contain CFC or HCFC. This grade i.. |
|||
Bulk Density | 0.590 - 0.630 g/cc | 0.0213 - 0.0228 lb/in³ | |
Polimeri Europa Extir Leonardo A 2000 AE Expandable Polystyrene
(discontinued **) Extir A 2000 AE is a flame retardant expandable polystyrene in the form of spherical beads of fine particle size, containing pentane as blowing agent. Extir does not contain CFC or HCFC. Extir A 200.. |