Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polimeri Europa SINKRAL G523 ABS, High Impact  (discontinued **)

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), Impact Grade, Molded
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF Polimeri Europa SINKRAL G523 ABS, High Impact  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
High impact; good flow; high gloss.Information provided by EnichemPolimeri Europa now has Enichem's plastics businesses. This grade is no longer in the product line.
Physical Properties Metric English Comments
Density 1.04 g/cc
0.0376 lb/in³
ASTM D792
Linear Mold Shrinkage 0.0040 cm/cm
0.0040 in/in
ASTM D955
Melt Flow 5.0 g/10 min

@Load 3.80 kg,
Temperature 230 °C
5.0 g/10 min

@Load 8.38 lb,
Temperature 446 °F
Cond. I; ASTM D1238
18 g/10 min

@Load 10.0 kg,
Temperature 220 °C
18 g/10 min

@Load 22.0 lb,
Temperature 428 °F
ISO 1133
Mechanical Properties Metric English Comments
Hardness, Rockwell R 105
105
ASTM D785
Tensile Strength, Yield 40.7 MPa
5900 psi
ASTM D638
Elongation at Break 50 %
50 %
ASTM D638
Flexural Modulus 2.73 GPa
396 ksi
ASTM D790
Izod Impact, Notched 3.70 J/cm

@Thickness 3.17 mm
6.93 ft-lb/in

@Thickness 0.125 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 1.8 MPa (264 psi) 99.0 °C
210 °F
Annealed; ASTM D648
Vicat Softening Point 104 °C
219 °F
ASTM D1525
Flammability, UL94 HB
HB
1/8 inch
HB
HB
1/16 inch