Material Notes:
Moplen EP500N is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP500N is a block copolymer particularly suitable for injection molding of containers, parts of electrical appliances, crates and pails. Moplen EP500N meets the FDA requirement in the code of Federal Regulations in 21 CFR 177.1520. And the components of additives are adequate on the food packaging substances specification of FDA regulation 21 CFR 178.2010.Features: Optimized balance of stiffness and toughness; High impact strength even at low temperature; Narrow molecular weight distribution; Low warpage; High whiteness; High glossApplications: Parts of electrical appliances; Pail; Housewares; Furniture (Chairs)Information provided by PolyMirae Company Ltd.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 95
95
ASTM D785
Tensile Strength, Yield 26.5 MPa
3840 psi
ASTM D638
Elongation at Yield 10 %
10 %
ASTM D638
Flexural Modulus 1.13 GPa
164 ksi
ASTM D790
Izod Impact, Notched 0.490 J/cm

@Temperature -20.0 °C
0.918 ft-lb/in

@Temperature -4.00 °F
ASTM D256
0.981 J/cm

@Temperature 23.0 °C
1.84 ft-lb/in

@Temperature 73.4 °F
ASTM D256
Users viewing this material also viewed the following: