Mechanical Properties | Metric | English | Comments |
---|---|---|---|
Izod Impact, Notched | 0.490 J/cm @Temperature 23.0 °C |
0.918 ft-lb/in @Temperature 73.4 °F |
ASTM D 256 |
SABIC Innovative Plastics Geloy XTWE480 ASA (Asia Pacific) Anti-scratch Geloy grade with excellent weatherability, high flow, and good surface quality. XTWE480 is available in various colours.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Izod Impact, Notched | 0.490 J/cm @Temperature -20.0 °C |
0.918 ft-lb/in @Temperature -4.00 °F |
|
PolyMirae Moplen EP300K Injection Molding Grade Polypropylene Moplen EP300K is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP300K is a block copolymer particularly suitable for injection.. |
|||
Izod Impact, Notched | 0.490 J/cm @Temperature -20.0 °C |
0.918 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
PolyMirae Moplen EP300R Injection Molding Grade Polypropylene Moplen EP300R is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP300R is a block copolymer particularly suitable for injection.. |
|||
Izod Impact, Notched | 0.490 J/cm @Temperature -20.0 °C |
0.918 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
PolyMirae Moplen EP500N Injection Molding Grade Polypropylene Moplen EP500N is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP500N is a block copolymer particularly suitable for injection.. |
|||
Izod Impact, Notched | 0.490 J/cm @Temperature 23.0 °C |
0.918 ft-lb/in @Temperature 73.4 °F |
ASTM D256 |
PolyMirae Moplen RP344R Injection Molding Grade Polypropylene Moplen RP344R is a nucleated polypropylene random copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen RP344R is a random copolymer particularly suitable for.. |
|||
Izod Impact, Notched | 0.490 J/cm @Temperature -20.0 °C |
0.918 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
PolyMirae Moplen EP641P Injection Molding Grade Polypropylene Moplen EP641P is the polypropylene block copolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen EP641P is a block copolymer suitable for injection molding of c.. |
|||
Izod Impact, Notched | 0.490 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
0.918 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical ALPHALAC SG970 HIPS Description: Injection Molding, General Purpose, Good Processability, High glossApplication: Air Conditioner Panel, Washer CoverCAS No. 9003-55-8Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.490 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
0.918 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical HIPS 403AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Electric Parts Requiring Flame RetardancyCAS: 9003-55-8, 21850-44-2 and 1309-64-4Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.490 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
0.918 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical HIPS 406AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Office Appliances (Parts of Printer or Copier)CAS: 9003-55-8, 25713-60-4 and 1309-64-4Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.490 J/cm @Thickness 6.40 mm, Temperature -30.0 °C |
0.918 ft-lb/in @Thickness 0.252 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical HIPS 410AF PS, Flame Retardant Description: Injection Molding, PS, Flame RetardantApplication: Office Appliances (Parts of Printer or Copier)CAS: 9003-55-8, 25713-60-4 and 1309-64-4Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.490 J/cm @Thickness 6.40 mm, Temperature -30.0 °C |
0.918 ft-lb/in @Thickness 0.252 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical HIPS 60HRI PS, Impact Modified Description: Injection Molding, PS, General Purpose, Impact ModifiedApplication: TV Sets, Tape Recorders, Vacuum Cleaner, Washing Machine, Air ConditionerCAS: 9003-55-8Information provided by LG Che.. |
|||
Izod Impact, Notched | 0.490 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
0.918 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical HIPS MI770 PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
Izod Impact, Notched | 0.490 J/cm @Thickness 6.40 mm, Temperature -30.0 °C |
0.918 ft-lb/in @Thickness 0.252 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical HIPS MI770 PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
Izod Impact, Notched | 0.490 J/cm @Thickness 6.40 mm, Temperature -40.0 °C |
0.918 ft-lb/in @Thickness 0.252 in, Temperature -40.0 °F |
ASTM D256 |
LG Chemical KEYFLEX BT 1072D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Injection Parts for Automotives, Leisure & SportsCAS: 37282-12-5Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.490 J/cm @Thickness 6.40 mm, Temperature -40.0 °C |
0.918 ft-lb/in @Thickness 0.252 in, Temperature -40.0 °F |
ASTM D256 |
LG Chemical KEYFLEX BT 1172D Ester Type TPE Description: Injection Molding, TPC-ET, General Purpose, High ModulusApplication: Cable & Wire Jackets, Hose & Tubing, SheetCAS: 37282-12-5Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.490 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
0.918 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical LI931 Extrusion ASA Description: Low Gloss, Extrusion Application: Industrial Materials (Window Profile, Tile Etc)CAS: 26299-47-8 & 9003-54-7Information provided by LG Chemical |
|||
Izod Impact, Notched | >= 0.490 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
>= 0.918 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical LUPOL HF5254A PP+MF20% Description: Injection Molding, PP+MF20%, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0 and 14807-96-6Information provided by LG Chemical |
|||
Izod Impact, Notched | >= 0.490 J/cm @Thickness 6.40 mm, Temperature -30.0 °C |
>= 0.918 ft-lb/in @Thickness 0.252 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical LUPOL HI4352L PP+Rubber+MF, High Impact Description: Injection Molding, PP+Rubber+MF, Good Dimensional Stability, High ImpactApplication: Automotive Exterior (Sill Side Molding, Door Garnish)CAS: 9003-07-0, 26221-73-8 and 14807-96-6Inform.. |
|||
Izod Impact, Notched | >= 0.490 J/cm @Thickness 6.40 mm, Temperature -10.0 °C |
>= 0.918 ft-lb/in @Thickness 0.252 in, Temperature 14.0 °F |
ASTM D256 |
LG Chemical LUPOL HI5302R PP+MF30%, High Impact Description: Injection Molding, PP+MF30%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 9010-79-1 and 14807-96-6Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.490 J/cm @Thickness 3.20 mm, Temperature -30.0 °C |
0.918 ft-lb/in @Thickness 0.126 in, Temperature -22.0 °F |
ASTM D256 |
LG Chemical ALPHALAC SG970NSU HIPS Description: Injection Molding, General Purpose, Good Processability, High gloss, antistatic and UV stabilizedApplication: Air Conditioner Panel, Washer CoverCAS No. 9003-55-8Information provided by.. |
|||
Izod Impact, Notched | >= 0.490 J/cm @Thickness 6.40 mm, Temperature -10.0 °C |
>= 0.918 ft-lb/in @Thickness 0.252 in, Temperature 14.0 °F |
ASTM D256 |
LG Chemical LUPOL HM5204 PP+MF20%, High Impact Description: Injection Molding, PP+MF20%, High Impact, Good WeatherabilityApplication: Automotive Interior PartsCAS: 9003-07-0, 9010-79-1 and 14807-96-6Information provided by LG Chemical |
|||
Izod Impact, Notched | 0.490 J/cm @Thickness 3.17 mm |
0.918 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® GP-5150GT PBT, 15% Glass Filled Low warpage with 15% GF reinforcement and can be used in the switches for microwave or ovensInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.490 J/cm @Thickness 3.17 mm |
0.918 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Starex® TF-0956 HI-PMMA Information provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.490 J/cm @Thickness 3.17 mm |
0.918 ft-lb/in @Thickness 0.125 in |
ASTM D256 |
Samsung Cheil Industries Infino® GP-5150GT PBT, 15% Glass Filled Low warpage with 15% GF reinforcement and can be used in the switches for microwave or ovensInformation provided by Samsung Cheil Industries. |
|||
Izod Impact, Notched | 0.490 J/cm @Temperature -20.0 °C |
0.918 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
SCG Chemicals EL-Proâ„¢ P440J Polypropylene Injection Molding Key Characteristics:Excellent impact strengthSuitable for small to medium partsRecommended Applications:High impact and durable automotive, motorcycle and electrical appliance parts such as fan stan.. |
|||
Izod Impact, Notched | 0.490 J/cm @Temperature 0.000 °C |
0.918 ft-lb/in @Temperature 32.0 °F |
ASTM D256 |
SCG Chemicals EL-Proâ„¢ P640J Polypropylene Injection Molding Key Characteristics:Good flowabilityHigh stiffnessHigh impact strengthRecommended Applications:High impact electrical appliance parts, automotive and motorcycle parts such as fan stand, washing tubI.. |
|||
Izod Impact, Notched | 0.490 J/cm @Temperature -20.0 °C |
0.918 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
SCG Chemicals EL-Proâ„¢ P722JO Polypropylene Injection Molding Key Characteristics:Good flowabilityGood sealabilityGood mechanical property balanceMinimal shrinkage and warpageContains UV stabilizerRecommended Applications:Good impact automotive and electrical .. |
|||
Izod Impact, Notched | 0.490 J/cm @Thickness 6.40 mm |
0.918 ft-lb/in @Thickness 0.252 in |
ASTM D-256 |
Bhansali Engineering Abstron IMG1130 Glass Reinforced Grade Glass Reinforced ABS & SAN Resins for product specific requirement of very high rigidity and temperatureInformation provided by Bhansali |
|||
Izod Impact, Notched | 0.490 J/cm @Thickness 6.40 mm, Temperature 23.0 °C |
0.918 ft-lb/in @Thickness 0.252 in, Temperature 73.4 °F |
ASTM D256 |
LG Chemical HIPS MI750 PS, Impact Modified Description: Injection Molding, PS, Impact Modified, High GlossApplication: Electric/Electronic Components, Stationary Articles, Food Containers, etc.CAS: 9003-55-8Information provided by LG Chemica.. |
|||
Izod Impact, Notched | 0.490 J/cm @Temperature -20.0 °C |
0.918 ft-lb/in @Temperature -4.00 °F |
ASTM D256 |
SCG Chemicals EL-Pro™ P441JU Polypropylene Injection Molding Key Characteristics:Excellent impact strengthContains UV stabilizer and anti-static agentSuitable for small to medium partsRecommended Applications:High impact and durable automotive and electrical .. |