Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyMirae Moplen HF524J BDDP Film Grade Polypropylene

Category Polymer , Film , Thermoplastic , Polypropylene (PP) , Polypropylene, Film Grade
Manufacturer PolyMirae Company Ltd.
Trade Name Moplen
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyMirae Moplen HF524J BDDP Film Grade Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Moplen HF524J is the Addiform polypropylene. Compared to ordinary pelletized polypropylene, Addiform gives significant advantages in terms of improved productivity, better processing and lower energy consumption. End products have also been found to have superior characteristics when using Addiform in a number of application areas. Moplen HF524J is the homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. MIRAEPOL PA124VS is a homopolymer particularly suitable for BOPP (Tender). Moplen HF524J resin meets the FDA requirements in the Code of Federal Regulations in 21 CFR 178.2010 for food packaging substances with adequate additives. And contains no dangerous substances according to Federal Regulations in 21 CFR 177.1520.Features: High Transparency and Gloss; Excellent processability; High stiffness and strength; Good barrier property; Increasing output and low energy consumptionApplications: General purpose packaging; Lamination Film; Adhesive tape Information provided by PolyMirae Company Ltd.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 3.0 g/10 min

@Load 2.16 kg,
Temperature 230 °C
3.0 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 98
98
ASTM D785
Tensile Strength, Yield 36.3 MPa
5260 psi
ASTM D638
Elongation at Yield 12 %
12 %
ASTM D638
Flexural Modulus 1.57 GPa
228 ksi
ASTM D790
Izod Impact, Notched 0.490 J/cm
0.918 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 105 °C
221 °F
ASTM D648
Vicat Softening Point 153 °C
307 °F
ASTM D1525
Users viewing this material also viewed the following: