Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 153 °C | 307 °F | B |
Plastcom SLOVALEN PC 13 T 30 PP, 30% mineral filling FeaturesModified copolymer PP for injection moulding or extrusion parts with the content of 30 % mineral filler. Increased rigidity, strength and impact strenght.Delivered in natural mode and in the.. |
|||
Vicat Softening Point | 153 °C | 307 °F | ASTM D1525B |
SABIC PP 578P Polypropylene Homopolymer for Injection Molding Product Description: PP 578P is a controlled rheology PP grade of medium molecular weight distribution suitable for injection molding applications. It gives consistent processability, good flow pr.. |
|||
Vicat Softening Point | 153 °C | 307 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics Lexan® 141 PC (Europe-Africa-Middle East) LEXAN 141 is a medium viscosity multi purpose grade available in transparent, translucent and opaque colours. |
|||
Vicat Softening Point | 153 °C | 307 °F | Rate B/50; ASTM D 1525 |
SABIC Innovative Plastics Lexan® AD4820 PC LEXAN AD4820 is a high viscosity grade exhibiting low dust attraction with a UV cut-off up to 400 nm and greater optical purity than standard resin.This data was supplied by SABIC-IP for the America.. |
|||
Vicat Softening Point | 153 °C | 307 °F | Rate B/50; ASTM D1525 |
SABIC Innovative Plastics Lexan® AD4820 PC (Europe-Africa-Middle East) LEXAN AD4820 is a high viscosity grade exhibiting low dust attraction with a UV cut-off up to 400 nm and greater optical purity than standard resin. |
|||
Vicat Softening Point | 153 °C | 307 °F | ASTM D1525 |
PolyMirae Moplen HP524J BDDP Film Grade Polypropylene Moplen HP524J is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP524J is a homopolymer particularly suitable for BOPP (Tender) fil.. |
|||
Vicat Softening Point | 153 °C | 307 °F | ASTM D1525 |
PolyMirae Moplen HP525J BDDP Film Grade Polypropylene Moplen HP525J is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP525J is a homopolymer particularly suitable for Metallizable BOPP.. |
|||
Vicat Softening Point | 153 °C | 307 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics Lexan® HP4R PC Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). ETO and steam sterilizable. Contains a h.. |
|||
Vicat Softening Point | 153 °C | 307 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics Lexan® HP4R PC (Asia Pacific) Medium flow polycarbonate. For medical devices and pharmaceutical applications. Healthcare management of change, biocompatible (ISO10993 or USP Class VI). EtO and steam sterilizable. Contains a hig.. |
|||
Vicat Softening Point | 153 °C | 307 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics Lexan® 141R PC (Europe-Africa-Middle East) LEXAN 141R is a medium viscosity multi purpose grade and contains a release agent to ensure easy processing. LEXAN 141R is available in transparent, translucent and opaque colours. |
|||
Vicat Softening Point | 153 °C | 307 °F | ASTM D1525 |
PolyMirae Moplen HP425J BDDP Film Grade Polypropylene Moplen HP425J is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. MIRAEPOL T28C is a homopolymer particularly suitable for BOPP (Tender) fil.. |
|||
Vicat Softening Point | 153 °C | 307 °F | A120; ISO 306 |
Inno-Comp INNOPOL® CS 1-3000 N DEL Polypropylene Homopolymer INNOPOL® CS 1-3000 N DEL is developed for producing injection molded automotive components.All information provided by INNO-COMP. |
|||
Vicat Softening Point | 153 °C | 307 °F | A120; ISO 306 |
Inno-Comp INNOPOL® CS 1-2120 AP 20% Talc Filled Polypropylene Homopolymer INNOPOL CS 1-2120 AP is a 20 % talc filled compound based on polypropylene homopolymer. This grade is available in natural and custom colored form.INNOPOL® CS 1-2120 AP is recommended especially.. |
|||
Vicat Softening Point | 153 °C | 307 °F | Loading 1 (10N); ASTM D1525 |
Teknor Apex Sinpolene TPP1010 Polypropylene Availability: Africa & Middle East; Latin America; Asia Pacific; South America Talc Filler, 10% Filler by Weight Uses: Appliance Components; Housings Forms: Pellets Processing Method: Injection Mol.. |
|||
Vicat Softening Point | 153 °C | 307 °F | A (10N); ISO 306 |
Borealis Daplen™ HJ060UB Polypropylene Compound for Direct Left Manufactured Applications Daplen FJ060UB is a special low viscosity compound for direct LFT manufacturing process. It interacts perfectly with glass fibers to create excellent stiffness and impact resistance. Daplen HJ060U.. |
|||
Vicat Softening Point | 153 °C | 307 °F | 10N-50°C per hour; ISO 306 |
Total PPH 10042 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 10042 is a nucleated antistatic homopolymer. PPH 10042 is characterized by high fluidity for high speed injection of thin wall articles such as dairy pots and tubs, salad .. |
|||
Vicat Softening Point | 153 °C | 307 °F | 10N-50°C per hour; ISO 306 |
Total PPH 10060 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 10060 homopolymer. PPH 10060 is characterized by high fluidity and is particularly suitable for injection molding applications. The material provides a good balance betwe.. |
|||
Vicat Softening Point | 153 °C | 307 °F | 10N-50°C per hour; ISO 306 |
Total PPH 9069 Polypropylene, Homopolymer ATOFINA Polypropylene PPH 9069 is homopolymer.ApplicationATOFINA Polypropylene PPH 9069 is intended for applications in non-wovens. It is also suitable for extrusion of bulk continuous filament (BC.. |
|||
Vicat Softening Point | 153 °C | 307 °F | ASTM D1525 |
Toyobo PELPRENE™ P46D-01 Polyester TPE, High Viscous, High Durability Features: Polyester TPE, High Viscous, High DurabilityInformation provided by Toyobo. |
|||
Vicat Softening Point | 153 °C | 307 °F | ISO 306/A50 |
ExxonMobil PP1055E2 Polypropylene Homopolymer Product Description: A nucleated homopolymer resin with good flowability and antistatic properties. It is designed for molding of media packaging, containers and other articles requiring fast moldi.. |
|||
Vicat Softening Point | 153 °C | 307 °F | 10 N; ASTM D1525 |
Braskem H 301 Injection Molding Polypropylene Description: H 301 is a high melt flow rate homopolymer designed for injection moulding and fiber extrusion. This product exhibits excellent processability with good melt strength and stiffness/impa.. |
|||
Vicat Softening Point | 153 °C @Load 1.02 kg |
307 °F @Load 2.25 lb |
ASTM-D1525 |
Braskem PH 0242 HOMO Polypropylene Homopolymer PH 0242 is a low melt flow rate homopolymer produced by compression molding. This resin exhibits excellent processability and excellent stiffness/impact strength balance. Its applications include co.. |
|||
Vicat Softening Point | 153 °C | 307 °F | 50 N; ISO 306 |
Azoty Tarnow™ TARNOFORM 700 POM Easy flowing grade for injection molding of thin-walled parts or in case of long flow path.Information provided by Zakłady Azotowe w Tarnowie-Moscicach S.A. |
|||
Vicat Softening Point | 153 °C | 307 °F | ISO 306/A50 |
Addiplast Addilene H 490 M10F Flame Retardant Polypropylene, 10% Mineral Filled Flame retardant, mineral filled, with halogensInformation provided by Addiplast. |
|||
Vicat Softening Point | 153 °C | 307 °F | ISO 306/A50 |
Addiplast Addilene H 490 S Flame Retardant Polypropylene Flame retardant, unreinforced, with halogensInformation provided by Addiplast. |
|||
Vicat Softening Point | 153 °C | 307 °F | ISO 306/A50 |
Addiplast Addilene H 532 N30 Polypropylene Homopolymer Good surface appearanceInformation provided by Addiplast. |
|||
Vicat Softening Point | 153 °C | 307 °F | 50°C/hr, 50N; ISO 306 |
Teijin Panlite® G-3430R Glass Fiber Reinforced Polycarbonate Resin GF 30% reinforced and mold release grade, meeting UL 94 V-2.Applications:Mechanical, electric and electronic components that need mechanical property e.g., stiffnessPrecision machinery components th.. |
|||
Vicat Softening Point | 153 °C | 307 °F | Rate A/50; ISO 306 |
SABIC Innovative Plastics Lexan® 144 PC (Europe-Africa-Middle East) LEXAN 144 is a medium viscosity multi purpose grade. FDA food contact compliant in limited colors. |
|||
Vicat Softening Point | 153 °C @Load 1.02 kg |
307 °F @Load 2.25 lb |
ASTM-D1525 |
Braskem CP 404XP HECO Polypropylene Heterophasic Copolymer CP 404XP is a medium melt flow rate heterophasic copolymer with suitable additives to produce caps and closures for carbonated beverages. This product exhibits high stiffness and impact strength bal.. |
|||
Vicat Softening Point | 153 °C | 307 °F | -1kg; ASTM D1525 |
Braskem H 606 Thermoforming Polypropylene Description: H 606 is low melt flow rate homopolymer with general purpose additive package. This resin is designed for extrusion and thermoforming. H 606 presents excellent processability and high o.. |