PolyMirae Moplen HF600N Injection Molding Grade Polypropylene

Category Polymer , Thermoplastic , Polypropylene (PP) , Polypropylene, Molded
Manufacturer PolyMirae Company Ltd.
Trade Name Moplen
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyMirae Moplen HF600N Injection Molding Grade Polypropylene.pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Moplen HF600N is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HF600N is a homopolymer with improved productivity and lower energy consumption and particularly suitable for injection molding of houseware articles, containers and general purpose. Moplen HF600N is an ADDIFORM homopolymer, ADDIFORM is the new controlled morphology polypropylene and is not palletized. Compared to ordinary palletized polypropylene, ADDIFORM gives considerable advantages in productivity, processing and energy consumption. Moplen HF600N resin meets the FDA requirements in the Code of Federal Regulations in 21 CFR 178.2010 for food packaging substances with adequate additives. And contains no dangerous substances according to Federal Regulations in 21 CFR 177.1520. Features: Reduce cycle time, considerable energy saving; Better color dispersion and lower consumption of color masterbatchesApplications: Containers; General houseware articles Information provided by PolyMirae Company Ltd.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 12.5 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12.5 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 104
104
ASTM D785
Tensile Strength, Yield 34.3 MPa
4980 psi
ASTM D638
Elongation at Yield 12 %
12 %
ASTM D638
Flexural Modulus 1.57 GPa
228 ksi
ASTM D790
Izod Impact, Notched 0.294 J/cm
0.551 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 107 °C
225 °F
ASTM D648