Physical Properties | Metric | English | Comments |
---|---|---|---|
Melt Flow | 12.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
12.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
Condition L; ASTM D1238 |
PolyMirae Moplen HF600N Injection Molding Grade Polypropylene Moplen HF600N is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HF600N is a homopolymer with improved productivity and lower energy.. |
|||
Melt Flow | 12.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
12.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® IFX3420Z PC (Asia Pacific) Lexan* IFX3420Z is a medium viscosity, release containing, injection moldable, polycarbonate grade suitable for use in industry protective eye-ware welding applications. This grades meets the transm.. |
|||
Melt Flow | 12.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
12.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® IFX5420Z PC (Asia Pacific) Lexan* IFX5420Z is a medium viscosity, release containing, injection moldable polycarbonate grade suitable for use in industry protective eye-ware welding applications. This grade meets the transmis.. |
|||
Melt Flow | 12.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
12.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® OQ2320 PC Ophthalmic/safety lens market. OQ2xxx series in all transparent tints. Dedicated equipment, stringent quality production control.This data was supplied by SABIC-IP for the Americas region. |
|||
Melt Flow | 12.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
12.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D 1238 |
SABIC Innovative Plastics Lexan® OQ2320 PC (Asia Pacific) Ophthalmic/safety lens market. OQ2xxx series in all transparent tints. Dedicated equipment, stringent quality production control.This data was supplied by SABIC-IP for the Asia Pacific region. |
|||
Melt Flow | 12.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
12.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics Lexan® OQ4320R PC (Asia Pacific) Optical grade with UV cut-off up to 400 nm; greater optical purity than standard grades. For sunglass and sunvisor markets. Internal mold release. |
|||
Melt Flow | 12.5 g/10 min | 12.5 g/10 min | Condition G |
Ineos Nova 3601 General Purpose Crystal Polystyrene
(discontinued **) Easy flow for high productivity, excellent post molding scuff resistanceApplications: Medical, LabwareExposure to gamma radiation in the 2.02-6.06 megarad range has no significant effect on the phys.. |
|||
Melt Flow | 12.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
12.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Eastman E6838-850P Polyethylene
(discontinued **) E6838-850P is a low density resin designed for applications where high coating speeds and good drawdown are required. The combination of high melt index and low density also provides good heat seal.. |
|||
Melt Flow | 12.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
12.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
NOVA Chemicals Novapol® HE-D250A HDPE Extrusion Resin
(discontinued **) Features: Excellent ESCR and toughness, good processability.Applications: conduit, corrugated pipe.Data provided by the manufacturer. |
|||
Melt Flow | 12.5 g/10 min @Load 5.00 kg, Temperature 300 °C |
12.5 g/10 min @Load 11.0 lb, Temperature 572 °F |
|
Hybrid Plastics PO6C81.01 Nanoreinforced® Polyphenylene Oxide (PPO) PPO available on the market today is typically mixed with polystyrene or other polymers to make it processable. However, these resins degrade the excellent mechanical and flammability properties of .. |
|||
Melt Flow | 12.5 g/10 min @Load 21.6 kg, Temperature 190 °C |
12.5 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Ineos K44-15-186 Polyethylene Copolymer K44-15-186 is a blue high-density polyethylene copolymer designed specifically for extrusion of pipe by blending K44-15-122 natural resin with G38-70C BLU II concentrate or an approved equivalent. .. |
|||
Melt Flow | 12.5 g/10 min @Load 21.6 kg, Temperature 190 °C |
12.5 g/10 min @Load 47.6 lb, Temperature 374 °F |
ASTM D1238 |
Ineos K44-15-186 Polyethylene Copolymer K44-15-186 is a blue high-density polyethylene copolymer designed specifically for extrusion of pipe by blending K44-15-122 natural resin with G38-70C BLU II concentrate or an approved equivalent. I.. |
|||
Melt Flow | 12.5 g/10 min | 12.5 g/10 min | ASTM D1238 |
Lucky IF-850 Acrylic, Injection Grade Easy-flow injection molding grade. May be UV stabilized. General Lucky PMMA qualities: Transparent/elegant appearance, high heat and weather resistance, excellent chemical resistance and coloring .. |
|||
Melt Flow | 12.5 g/10 min @Load 6.60 kg, Temperature 367 °C |
12.5 g/10 min @Load 14.6 lb, Temperature 693 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM XH6050 PEI Copolymer Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Melt Flow | 12.5 g/10 min @Load 6.60 kg, Temperature 367 °C |
12.5 g/10 min @Load 14.6 lb, Temperature 693 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM XH6050 PEI Copolymer (Asia Pacific) Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Melt Flow | 12.5 g/10 min @Load 6.60 kg, Temperature 367 °C |
12.5 g/10 min @Load 14.6 lb, Temperature 693 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM XH6050F PEI Copolymer Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming. US FDA Compliant. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Melt Flow | 12.5 g/10 min @Load 6.60 kg, Temperature 367 °C |
12.5 g/10 min @Load 14.6 lb, Temperature 693 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM XH6050F PEI Copolymer (Asia Pacific) Transparent, enhanced flow Polyetherimidesulfone copolymer (Tg 247C). ECO Conforming. US FDA Compliant. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Melt Flow | 12.5 g/10 min @Load 6.60 kg, Temperature 367 °C |
12.5 g/10 min @Load 14.6 lb, Temperature 693 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM XH6050M PEI Copolymer Enhanced flow Polyetherimidesulfone copolymer (Tg 247C) with internal mold release. ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Melt Flow | 12.5 g/10 min @Load 5.00 kg, Temperature 280 °C |
12.5 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
Melt Flow | 12.5 g/10 min @Load 5.00 kg, Temperature 280 °C |
12.5 g/10 min @Load 11.0 lb, Temperature 536 °F |
ASTM D1238 |
SABIC Innovative Plastics NORYL GTX GTX944 PPE+PA (Asia Pacific) NORYL GTX944 is an unfilled GTX grade with improved processability and increased impact performance. |
|||
Melt Flow | 12.5 g/10 min @Load 6.60 kg, Temperature 367 °C |
12.5 g/10 min @Load 14.6 lb, Temperature 693 °F |
ASTM D1238 |
SABIC Innovative Plastics ULTEM XH6050M PEI Copolymer (Asia Pacific) Enhanced flow Polyetherimidesulfone copolymer (Tg 247C) with internal mold release. ECO Conforming, UL94 V0 listing. Resin is subject to U.S. Commerce Control Laws (15CFR Chapter VII, Part 774). |
|||
Melt Flow | 12.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
12.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics XYLEX X7519HP PC+POLYESTER Good Chemical Resistance, XYLEX grade with good dishwasher performance, USA/Europe Food Contact Comment: While molding of thicker parts, cooling speed has an influence of transparency. Thicker parts.. |
|||
Melt Flow | 12.5 g/10 min @Load 1.20 kg, Temperature 300 °C |
12.5 g/10 min @Load 2.65 lb, Temperature 572 °F |
ASTM D1238 |
SABIC Innovative Plastics XYLEX X7519HP PC+POLYESTER (Asia Pacific) Good Chemical Resistance, XYLEX grade with good dishwasher performance, USA/Europe Food Contact Comment: While molding of thicker parts, cooling speed has an influence of transparency. Thicker parts.. |
|||
Melt Flow | 12.5 g/10 min @Load 2.16 kg, Temperature 230 °C |
12.5 g/10 min @Load 4.76 lb, Temperature 446 °F |
ISO 1133 |
Borealis Steripeel™ WE150CF PO Compound for Sterilizable Peelable Film Applications Steripeel WE150CF is a slip and antiblock agent formulated film resin. It is suitable for the manufacturing of unoriented peelable cast films on chill roll process.Steripeel WE150CF is suitable for.. |
|||
Melt Flow | 12.5 g/10 min @Load 2.16 kg, Temperature 190 °C |
12.5 g/10 min @Load 4.76 lb, Temperature 374 °F |
ASTM D1238 |
Westlake EC850AA Low Density Polyethylene WESTLAKE low-density polyethylene EC850 is a resin designed for applications where high coating speeds and good drawdown are required. The combination of high melt index and low density provides goo.. |
|||
Melt Flow | 12.5 g/10 min @Load 6.60 kg, Temperature 367 °C |
12.5 g/10 min @Load 14.6 lb, Temperature 693 °F |
ASTM D1238 |
Westlake Plastics Tempalux® 5000 Polyetherimide An amorphous thermoplastic polyetherimide, stock shapes from ULTEM® resin possess a combination of useful characteristics, including high heat resistance, high strength at elevated temperatures, hi.. |
|||
Melt Flow | 12.5 g/10 min | 12.5 g/10 min | ASTM D1238 |
Asahi Kasei Thermylene® P6-35FM-1309 35% Glass and Mineral Reinforced, Heat Stabilized Information provided by Asahi Thermofil |