Moplen HP526N is the polypropylene homopolymer manufactured by PMC under the license of BASELL using the Spheripol process. Moplen HP526N is a homopolymer particularly suitable for WQB (Water Quenching Blown) film. Moplen HP526N resin meets the FDA requirements in the Code of Federal Regulations in 21 CFR 178.2010 for food packaging substances with adequate additives. And contains no dangerous substances according to Federal Regulations in 21 CFR 177.1520.Features: High Transparency and gloss; High slip and antiblocking; High stiffness; Good sealability Applications: Packaging; Foodstuffs; Stationary items Information provided by PolyMirae Company Ltd.
Physical Properties Metric English Comments
Density 0.900 g/cc
0.0325 lb/in³
ASTM D1505
Melt Flow 12 g/10 min

@Load 2.16 kg,
Temperature 230 °C
12 g/10 min

@Load 4.76 lb,
Temperature 446 °F
Condition L; ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Rockwell R 101
101
ASTM D785
Tensile Strength, Yield 34.3 MPa
4980 psi
ASTM D638
Elongation at Yield 12 %
12 %
ASTM D638
Flexural Modulus 1.52 GPa
220 ksi
ASTM D790
Izod Impact, Notched 0.392 J/cm
0.735 ft-lb/in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 105 °C
221 °F
ASTM D648
Vicat Softening Point 155 °C
311 °F
ASTM D1525