Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Dynaflex™ D3226-1000-03 Thermoplastic Elastomer (TPE)

Category Polymer , Thermoplastic , Elastomer, TPE
Manufacturer PolyOne Corporation
Trade Name Dynaflex™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Dynaflex™ D3226-1000-03 Thermoplastic Elastomer (TPE).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Dynaflex™ D3226-1000-03 is an easy processing TPE designed for general purpose applications. It is suitable for injection molding, extrusion, blow molding and thermoforming processes. - Dry Feel - Easy Processing - Good Melt Strength - Soft TouchColor concentrates ethylene vinyl acetate (EVA) carriers are most suitable for coloring Dynaflex™ D3226-1000-03. Improved color dispersion can be achieved by using higher melt flow concentrates (with a melt flow rate of 25 - 40 g/10 min). Typical loadings for color concentrates are 1% to 5% by weight. A high color match consistency may be obtained by using precolored compounds available from GLS. Concentrates based on PVC should not be used. The final determination of color concentrate suitability should be determined by customer trials. Purge thoroughly before and after use of this product with a low flow (0.5 - 2.5 MFR) polystyrene (PS) or polypropylene (PP). Dynaflex™ D3226-1000-03 has good melt stability. Maximum residence times may vary, depending on the size of the barrel. Generally, the barrel should be emptied if it is idle for periods of 5 - 8 minutes or longer. Drying is not Required Injection Speed: 1 to 5 in/sec 1st Stage - Boost Pressure: 200 to 600 psi 2nd Stage - Hold Pressure: 70% of Boost Hold Time (Thick Part): 4 to 10 sec Hold Time (Thin Part): 1 to 3 secInformation provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 0.988 g/cc
0.988 g/cc
ASTM D792
Linear Mold Shrinkage, Flow 0.0020 - 0.0060 cm/cm
0.0020 - 0.0060 in/in
ASTM D955
Melt Flow 26 g/10 min

@Load 2.16 kg,
Temperature 190 °C
26 g/10 min

@Load 4.76 lb,
Temperature 374 °F
ASTM D1238
82 g/10 min

@Load 5.00 kg,
Temperature 200 °C
82 g/10 min

@Load 11.0 lb,
Temperature 392 °F
ASTM D1238
Mechanical Properties Metric English Comments
Hardness, Shore A 40
40
10 sec; ASTM D2240
Tensile Strength at Break 3.59 MPa

@Temperature 23.0 °C
521 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
Tensile Stress 2.96 MPa

@Strain 100 %,
Temperature 23.0 °C
429 psi

@Strain 100 %,
Temperature 73.4 °F
Die C2 hr; ASTM D412
Elongation at Break 380 %

@Temperature 23.0 °C
380 %

@Temperature 73.4 °F
Die C2 hr; ASTM D412
Tear Strength 15.8 kN/m
90.2 pli
ASTM D624
Compression Set 15 %

@Temperature 23.0 °C,
Time 79200 sec
15 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395B
Processing Properties Metric English Comments
Rear Barrel Temperature 154 - 193 °C
309 - 379 °F
Middle Barrel Temperature 160 - 199 °C
320 - 390 °F
Front Barrel Temperature 166 - 204 °C
331 - 399 °F
Nozzle Temperature 166 - 204 °C
331 - 399 °F
Mold Temperature 21.1 - 32.2 °C
70.0 - 90.0 °F
Back Pressure 0.345 - 1.03 MPa
50.0 - 149 psi
Screw Speed 25 - 75 rpm
25 - 75 rpm
Descriptive Properties Value Comments
Agency Ratings FDA Unspecified Rating
Appearance Natural Color
Features Good Melt Strength
Good Processability
Forms Pellets
Generic Material TPE
Generic Name Thermoplastic Elastomer (TPE)
Manufacturer / Supplier GLS Thermoplastic Elastomers
Processing Method Extrusion
Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
RoHS Compliance RoHS Compliant
Uses Consumer Applications
General Purpose
Toys
Users viewing this material also viewed the following: