Processing Properties | Metric | English | Comments |
---|---|---|---|
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products F4900-611UV Thermoplastic Polyolefin, UV Stabilized, XS9 Dark Neutral Metallic Applications: Exterior componentsBodyside moldingsStep padsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products F55-01 43% Glass Fiber/Talc Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Consumer goodsSupportsGolf cart bracketsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products F56-01 40% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black Applications: Consumer goodsUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products FT2500-01A Thermoplastic Polyolefin, Non-UV Stabilized, Black Applications: Air DamsHitch padsScuff platesInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products FT4700-00A Thermoplastic Polyolefin, Non-UV Stabilized, Natural Applications: CladdingsBodyside moldingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products G10UP100-01 10% Glass Fiber Reinforced Polypropylene, Black, UL94-HB Rated Applications: Consumer housingsConsumer goodsFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products G13P100-347UV 13% Glass Fiber Reinforced Polypropylene, UV Stabilized, 109D Medium Pewter Applications: Dome lamp housingsFuel filler pocketInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products GC45P200-01UV 45% Glass Fiber Reinforced Polypropylene Copolymer, UV Stabilized, Black Applications: BracketsUnderhood componentsLarge structural supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products HP514-489 14% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, 101E Lite Oak Applications: Glove box binInterior trimSteering column trimConsolesAir ducts - distributionInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products HP519-01 26% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Black Applications: Interior trim moldingsSill platesAir ductsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products HP531-680UV 22% Talc Reinforced High Performance Polypropylene Copolymer, UV Stabilized, Medium Scratch Resistant, BJAA Light Parchment Applications: I/P componentsInterior trimA/B/C/ PillarsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products M25UVP250-01 25% Mica Reinforced Polypropylene Copolymer, UV Stabilized, Black Applications: BracketsCowl screensRigid exterior componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products P250-247 Polypropylene Copolymer, UV Stabilized, Black Applications: Center consolesInterior trimI/P componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products RCT140-01A 40% Talc Reinforced Polypropylene, Black, Recycled Content Applications: HVAC ductworkI/P componentsFuse panel assembliesUnderhood componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products T20P100-01EG 20% Talc Reinforced Polypropylene, General Purpose Black, Extrusion Grade Applications: Consumer goodsAutomotive componentsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products T40P108-01A 40% Talc Reinforced Polypropylene, Black Applications: Underhood componentsHVAC ductworkFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.483 - 1.03 MPa | 70.0 - 150 psi | |
Ravago Manufacturing Americas Hylex® P1307L Polycarbonate Entec's proprietary products include a full range of compounds in the Nylon 6/6, Nylon 6, ABS, PBT, Polycarbonate, PC/ABS, PC/ASA, PC/PBT, and PPO/PPE resin families.Information provided by Ente.. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 149 psi | |
PolyOne Dynaflex™ G7410-1000-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7410-1000-00 is an easy processing, high performance compound designed for use in applications requiring a tough, durable material. - Excellent Colorability - Excellent Heat Stability - .. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 149 psi | |
PolyOne Dynaflex™ G7430-9001-00 Thermoplastic Elastomer (TPE) Dynaflex™ G7430-9001-00 is an easy processing, high performance compound designed for use in applications requiring tough, durable material. - Excellent Heat Stability - Good Ozone and UV Stability.. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products F15-00UV 35% Glass Fiber Reinforced Polypropylene, Chemically Coupled, UV-Stabilized, Natural Applications: Functional SupportsElectrical housingsConsumer GoodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products F32-01 32% Glass Fiber/Mineral Co-Reinforced Polypropylene, Chemically Coupled, Black Applications: Head lamp housingBracketsUnderhood componentsElectrical housingsFunctional supportsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products F35-01 35% Glass Fiber/Mineral Co-Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Interior trimUnderhood componentsConsumer goodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products HP506-01A 21% Talc Reinforced High Performance Polypropylene, UV Stabilized, Black Applications: Automotive interior applicationsHVAC ductsTail lamp housingsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products M12P256-01 12% Mica Reinforced Polypropylene Copolymer, Black Applications: Air damsAir ducts - distributionClose out panelsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 149 psi | |
PolyOne Dynaflex™ G7970-9001-02 Thermoplastic Elastomer (TPE) Dynaflex™ G7970-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications, including those where FDA compliance is required. - Overmold Adhesion to Polypropylen.. |
|||
Back Pressure | 0.000 - 1.03 MPa | 0.000 - 150 psi | |
MRC Polymers MAXTELâ„¢ 600T25 TPO, 25% Talc Filled For automotive exterior applicationsExcellent process ability and dimensional stabilityCan be UV StabilizedInternal and external lubricants can be addedInformation provided by MRC Polymers Inc. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
CTC SunPro® SP 200 P4058 Polypropylene Copolymer SunPro® SP 200 P 4058 is a general purpose, medium flow, polypropylene copolymer. It has applications in automotive wheel housings and general purpose automotive. Automotive Certifications: Chrysl.. |
|||
Back Pressure | 0.517 - 1.03 MPa | 75.0 - 150 psi | |
Diamond Polymers ASA T-110 Description: ASA Weatherable Polymer, Injection Molding Grade, Medium Heat ResistanceInformation provided by Diamond Polymers, Inc. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products GC43P250-01 43% Glass Fiber Reinforced Polypropylene Copolymer, Chemically Coupled, Black Applications: Consumer goodsFunctional supportsHead lamp bracketsDurable GoodsInjection molding conditions reported in table.Information provided by RheTech Products. |
|||
Back Pressure | 0.345 - 1.03 MPa | 50.0 - 150 psi | |
RheTech Products M20P100-01A 20% Mica Reinforced Polypropylene, Black Applications: Fan shroudsFiller panelsAir ductsInjection molding conditions reported in table.Information provided by RheTech Products. |