Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Edgetek® AS- 08CF / 000 ABS - 8% Carbon Fiber Reinforced With ESD Properties  (discontinued **)

Category Polymer , Thermoplastic , ABS Polymer , Acrylonitrile Butadiene Styrene (ABS), 10% Carbon Fiber Filled
Manufacturer
Trade Name
Port Shanghai port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Edgetek® AS- 08CF / 000 ABS - 8% Carbon Fiber Reinforced With ESD Properties  (discontinued **).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Data provided by PolyOne.
Physical Properties Metric English Comments
Density 1.08 g/cc
0.0390 lb/in³
ASTM D792
Water Absorption 0.25 %
0.25 %
24 hrs. ASTM D570
Linear Mold Shrinkage 0.0025 - 0.0040 cm/cm

@Thickness 3.17 mm
0.0025 - 0.0040 in/in

@Thickness 0.125 in
ASTM D955
Mechanical Properties Metric English Comments
Tensile Strength, Ultimate 79.0 MPa
11500 psi
ASTM D638
Elongation at Break 2.0 - 3.0 %
2.0 - 3.0 %
ASTM D638
Tensile Modulus 5.90 GPa
856 ksi
ASTM D638
Izod Impact, Notched 0.640 J/cm

@Thickness 6.35 mm
1.20 ft-lb/in

@Thickness 0.250 in
ASTM D256
Thermal Properties Metric English Comments
Deflection Temperature at 0.46 MPa (66 psi) 99.0 °C
210 °F
ASTM D648
Deflection Temperature at 1.8 MPa (264 psi) 96.0 °C
205 °F
ASTM D648
Electrical Properties Metric English Comments
Electrical Resistivity 10000 - 1.00e+6 ohm-cm
10000 - 1.00e+6 ohm-cm
ASTM D257
Surface Resistance 10000 - 1.00e+6 ohm
10000 - 1.00e+6 ohm
ASTM D257
Processing Properties Metric English Comments
Melt Temperature 221 - 249 °C
430 - 480 °F
Stock
Mold Temperature 27.0 - 54.0 °C
80.6 - 129 °F
Drying Temperature 77.0 °C
171 °F