PolyOne Geon™ Vinyl Flexible 90037 Polyvinyl Chloride, Flexible (PVC, Flexible)

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Flexible 90037 Polyvinyl Chloride, Flexible (PVC, Flexible).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Automotive OEM approval(s).Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.22 g/cc
1.22 g/cc
ASTM D792
Volatiles 0.34 %

@Thickness 1.91 mm,
Temperature 90.0 °C
0.34 %

@Thickness 0.0752 in,
Temperature 194 °F
Loss; Emery; ASTM D1203B
Mechanical Properties Metric English Comments
Hardness, Shore A 83
83
15 sec; ASTM D2240
Tensile Strength at Break 12.8 MPa
1860 psi
Type IV, 510 mm/min; ASTM D638
Elongation at Break 360 %
360 %
Type IV, 510 mm/min; ASTM D638
Tear Strength 50.0 kN/m
285 pli
Die C, 2 in/min; ASTM D1004
Descriptive Properties Value Comments
Automotive Specifications GM GMP.PVC.009
Features High Gloss
Forms Pellets
Fungal Resistance Pass
ASTM G21
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Low Temperature Flexibility Pass
-29°C, 508.0 µm; 4 hr, 12 mm
Processing Method Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Automotive Applications
Automotive Exterior Trim
Outdoor Applications
Xenon Weatherometer Pass
SAE J1960; Exterior, 2500 kJ/m², All Colors, dE*<3.0