Material Notes:
Automotive OEM approval(s).Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.25 g/cc
1.25 g/cc
ASTM D792
Volatiles 0.40 %

@Thickness 1.91 mm,
Temperature 105 °C
0.40 %

@Thickness 0.0752 in,
Temperature 221 °F
Loss; Method A; ASTM D1203B
Mechanical Properties Metric English Comments
Hardness, Shore D 37
37
15 sec; ASTM D2240
Tensile Strength at Break 22.0 MPa
3190 psi
Type IV, 510 mm/min; ASTM D638
Elongation at Break 290 %
290 %
Type IV, 510 mm/min; ASTM D638
Tear Strength 70.0 kN/m
399 pli
Die C, 2 in/min; ASTM D1004
Descriptive Properties Value Comments
Appearance Clear/Transparent
Automotive Specifications GM GMP.PVC.003
Features High Gloss
Forms Pellets
Fungal Resistance Pass
ASTM G21
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Low Temperature Flexibility Pass
-29°C, 508.0 µm; 4 hr, 12 mm
Processing Method Coextrusion
Extrusion
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Automotive Applications
Automotive Exterior Trim
Outdoor Applications
Xenon Weatherometer Pass
SAE J1960; Exterior, 2500 kJ/m², Natural, dE*<3.0