Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

PolyOne Geon™ Vinyl Flexible 90071 Polyvinyl Chloride, Flexible (PVC, Flexible)

Category Polymer , Thermoplastic , Vinyl (PVC)
Manufacturer PolyOne Corporation
Trade Name Geon™
Port Ningbo port,China
Trade Terms FOB, CFR, CIF
Payment Terms L/C, T/T, Western Union
Download PDF PolyOne Geon™ Vinyl Flexible 90071 Polyvinyl Chloride, Flexible (PVC, Flexible).pdf
Price EMAIL US    sales@lookpolymers.com
  Online Service   lookpolymers   27660005
Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.26 g/cc
1.26 g/cc
ASTM D792
Volatiles 0.34 %

@Thickness 1.91 mm,
Temperature 105 °C
0.34 %

@Thickness 0.0752 in,
Temperature 221 °F
Loss; Method A; ASTM D1203B
Mechanical Properties Metric English Comments
Hardness, Shore A 88
88
15 sec; ASTM D2240
Tensile Strength at Break 19.5 MPa
2830 psi
Type IV, 510 mm/min; ASTM D638
Elongation at Break 260 %
260 %
Type IV, 510 mm/min; ASTM D638
Tear Strength 65.0 kN/m
371 pli
Die C, 2 in/min; ASTM D1004
Descriptive Properties Value Comments
Features High Gloss
Forms Pellets
Fungal Resistance Pass
ASTM G21
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Low Temperature Flexibility Pass
-29°C, 508.0 µm; 4 hr, 12 mm
Processing Method Extrusion
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Automotive Applications
Automotive Exterior Trim
Beltline Moldings
Outdoor Applications
Xenon Weatherometer Pass
SAE J1960; Exterior, 2500 kJ/m², All Colors, dE*<3.0