Material Notes:
Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.39 g/cc
1.39 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 64
64
15 sec; ASTM D2240
70
70
ASTM D2240
Tensile Strength at Break 10.1 MPa
1460 psi
510 mm/min; ASTM D638
Tensile Strength 4.34 MPa

@Strain 100 %
629 psi

@Strain 100 %
510 mm/min; ASTM D638
Elongation at Break 390 %
390 %
510 mm/min; ASTM D638
Tear Strength 35.0 kN/m
200 pli
Die C, 510 mm/min; ASTM D624
Compression Set 20 %

@Temperature 23.0 °C,
Time 79200 sec
20 %

@Temperature 73.4 °F,
Time 22.0 hour
ASTM D395
Clash Berg Modulus 0.0814 GPa
11.8 ksi
ASTM D1043
0.310 GPa

@Temperature -46.0 °C
45.0 ksi

@Temperature -50.8 °F
ASTM D1043
Thermal Properties Metric English Comments
Brittleness Temperature -42.2 °C
-44.0 °F
ASTM D746
Flammability, UL94 HB
HB
UL 94
Processing Properties Metric English Comments
Melt Temperature 171 - 177 °C
340 - 351 °F
193 - 199 °C
379 - 390 °F
Descriptive Properties Value Comments
Agency Ratings NSF 51
NATURAL,BLACK 2999, WHITE 1300, WHITE 1380, BLUE 4060, GRAY 2000, GRAY 2600, GRAY 2604. Max. Temp.of use = 100 degrees F.
Features General Purpose
Medium Gloss
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Coextrusion
Extrusion
Injection Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses General Purpose
Seals