Material Notes:
XV3855 is a flexible (57A durometer) vinyl compound formulated from FDA-santioned raw materials. XV3855 Clear 1869 has been tested to USP Class VI.NOTE: All ingredients used in the formulation of this compound are listed in the United States FDA Code of Federal Regulations, Title 21. The only restriction is that the plasticizer is For foods of high water content only. This statement is only an overview of the FDA listings for this product. It is the customer's responsibility to ensure that the compound is suitable for its intended application.Information provided by PolyOne
Physical Properties Metric English Comments
Specific Gravity 1.16 g/cc
1.16 g/cc
ASTM D792
Mechanical Properties Metric English Comments
Hardness, Shore A 57
57
10 sec; ASTM D2240
Tensile Strength at Break 10.7 MPa
1550 psi
Type IV, 510 mm/min; ASTM D638
Tensile Strength 3.10 MPa

@Strain 100 %
450 psi

@Strain 100 %
Type IV, 510 mm/min; ASTM D638
Elongation at Break 490 %
490 %
Type IV, 510 mm/min; ASTM D638
Descriptive Properties Value Comments
Agency Ratings FDA Unspecified Rating
Appearance Clear/Transparent
Forms Pellets
Generic Material PVC, Flexible
Generic Name Polyvinyl Chloride, Flexible (PVC, Flexible)
Processing Method Blow Molding
Regional Availability Africa & Middle East
Asia Pacific
Europe
North America
South America
Uses Medical Appliances
Medical/Healthcare Applications
Users viewing this material also viewed the following: