Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Tensile Strength at Break = 1550 psi Product List

Mechanical Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Mechanical Properties Metric English Comments
Tensile Strength at Break 10.7 MPa
1550 psi
510 mm/min; ASTM D412A
PolyOne Synprene™ RT-5180 RoHS Natural Styrene Butadiene Block Copolymer (SBC)
Synprene™ thermoplastic elastomers (TPEs) are compounds based on styrenic block copolymer (SBC) technology, and can be formulated to deliver extremely low hardness values not found in other elastom..
Tensile Strength at Break 10.7 MPa

@Temperature 23.0 °C
1550 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Versaflex™ CL E85 Thermoplastic Elastomer (TPE)
Versaflex™ CL E85 is an exceptional clarity, high performance and autoclavable solution ideal for healthcare and food packaging. Versaflex™ CL E85 is also formulated without the use of plasticizer..
Tensile Strength at Break 10.7 MPa

@Temperature 23.0 °C
1550 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7990-1001-00 Thermoplastic Elastomer (TPE)
Dynaflex™ G7990-1001-00 is an easy processing, general purpose TPE designed for a wide variety of applications. - Overmold Adhesion to Polypropylene - Rubbery FeelDynaflex™ G7990-1001-00 can be re..
Tensile Strength at Break 10.7 MPa

@Temperature 23.0 °C
1550 psi

@Temperature 73.4 °F
Die C2 hr; ASTM D412
PolyOne Dynaflex™ G7990-9001-02 Thermoplastic Elastomer (TPE)
Dynaflex™ G7990-9001-02 is an easy processing, general purpose TPE designed for a wide variety of applications. - Overmold Adhesion to Polypropylene - Rubbery FeelDynaflex™ G7990-9001-02 can be re..
Tensile Strength at Break 10.7 MPa
1550 psi
Type IV, 510 mm/min; ASTM D638
PolyOne Geon™ Vinyl Flexible XV3855 Polyvinyl Chloride, Flexible (PVC, Flexible)
XV3855 is a flexible (57A durometer) vinyl compound formulated from FDA-santioned raw materials. XV3855 Clear 1869 has been tested to USP Class VI.NOTE: All ingredients used in the formulation of th..
Tensile Strength at Break 10.7 MPa
1550 psi
IEC 60811
Solvay Specialty Polymers Cogegum® AFR/930 Polyolefin, Unspecified  (discontinued **)
Cogegum® HFFR -Halogen Free Fire Retardant compound Polyolefin based thermoplastic compound containing a fire retardant system that contributes to give the cable self-extinguish properties without ..
Tensile Strength at Break 10.7 MPa
1550 psi
ASTM D1414
Greene Tweed CHEMRAZ® 571 Perfluoroelastomer
Chemraz® 571 is recommended for a wide variety of semiconductor equipment wet processing applications where stringent seal reliability and contamination control are required. This seal material ..
Tensile Strength at Break 10.7 MPa
1550 psi
Shin-Etsu Silicones KEP-12 Silicone additive
KEP12 is an additive which can be used in most of the silicone products to improve heat stability.Product Features: Improve thermal stability and compression set.Excellent dispersion.Information Pro..
Tensile Strength at Break 10.7 MPa
1550 psi
ASTM D412
Teknor Apex APEX® 2060-H Polyvinyl Chloride, Flexible
Material Status-Commercial: ActiveAvailability-North AmericaTest Standards Available-ASTMFeatures-Good FlexibilityUses-General Purpose, ProfilesAppearance-ClearForms-PelletsProcessing Method-Extrusi..
Tensile Strength at Break 10.7 MPa
1550 psi
ASTM D638
Teknor Apex APEX® 76-5179-B Polyvinyl Chloride, Flexible
Notes: 80°C General Purpose; RoHS Compliant Features: Flame Retardant Uses: Wire and Cable ApplicationsForms: Pellets Processing Method: Injection Molding Agency Ratings: UL QMFZ2 .E54709Addition..
Tensile Strength at Break 10.7 MPa
1550 psi
ASTM D638
Teknor Apex APEX® 87-L417D-NT Polyvinyl Chloride, Flexible
Notes: RoHS Compliant Forms: PelletsInformation Provided by Teknor Apex
Tensile Strength at Break 10.7 MPa
1550 psi
ASTM D638
Teknor Apex APEX® 90-A471R-60-NT Polyvinyl Chloride, Flexible
Features: DEHP Plasticizer; Radiation (Gamma) Resistant; Radiation Sterilizable Uses: Medical/Healthcare Applications; Tubing Processing Method: Extrusion Forms: PelletsInformation Provided by Tekno..
Tensile Strength at Break 10.7 MPa
1550 psi
ASTM D638
Teknor Apex HFFR 2003 Polyolefin, Halogen Free
Notes: RoHS Compliant Features: Flame Retardant; Halogen Free Uses: Communication Wire Jacketing; Electronic Cable Jacketing; Security Cable Jacketing; Fiber Optic Cable Agency Ratings: IEC 60332-1;..
Tensile Strength at Break 10.7 MPa
1550 psi
DBPH Cure
Shin-Etsu Silicones KE-5551U High Strength Silicone Elastomer
ShinEtsu KE5551 U is a nominal 50 Durometer base which offers high tensile and tear strengths. Its excellent processing characteristics make it suitable for molding, extrusion and calendaringProduct..
Tensile Strength at Break 10.7 MPa
1550 psi
20 in/min; ASTM D412
Teknor Apex Telcar® TL-1934E Styrenic Thermoplastic Elastomer
Uses: Appliance Wire Insulation; Cable Jacketing; Flexible Cord Insulation; Wire and Cable Applications; Wire Jacketing Agency Ratings: UL 1581 Forms: Pellets Processing Method: Extrusion; Injection..
Tensile Strength at Break 10.7 MPa
1550 psi
ASTM D638
Westlake Elevate™ EF526 16% Ethylene Vinyl Acetate Copolymer
Westlake Elevate™ EF526 resin is a 16% EVA copolymer designed for cast film, extrusion coatings, and thermal laminations.Application/UsesThermal laminationsCast FilmExtrusion CoatingsThis resin gra..
Tensile Strength at Break 10.7 MPa
1550 psi
ASTM D3759
3M Scotch® 356 Transparent Label Protection Tape
Scotch® Label Protection Tape 356 is a transparent, tough film tape made especially for label protection in outdoor applications or where the application demands extra resistance to moisture, chemi..
Copyright © lookpolymers.com All Rights Reserved